Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.221 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.37 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 103026 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.000 164.8
CsI (mp-614603) <1 1 0> <1 1 0> 0.000 174.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.006 164.8
BN (mp-984) <0 0 1> <1 1 1> 0.013 71.4
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.027 247.2
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.028 285.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.031 116.5
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.033 285.5
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.034 71.4
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.035 164.8
KCl (mp-23193) <1 0 0> <1 0 0> 0.035 41.2
Ge (mp-32) <1 0 0> <1 0 0> 0.038 164.8
KCl (mp-23193) <1 1 0> <1 1 0> 0.038 58.3
KCl (mp-23193) <1 1 1> <1 1 1> 0.039 71.4
GaN (mp-804) <0 0 1> <1 0 0> 0.041 288.4
C (mp-66) <1 0 0> <1 0 0> 0.041 164.8
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.044 174.8
C (mp-66) <1 1 1> <1 1 1> 0.045 285.5
ZnO (mp-2133) <0 0 1> <1 0 0> 0.048 329.6
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.065 174.8
Al (mp-134) <1 0 0> <1 0 0> 0.068 82.4
MgO (mp-1265) <1 0 0> <1 0 0> 0.074 164.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.076 329.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.080 233.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.091 82.4
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.107 329.6
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.112 233.1
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.112 71.4
Mg (mp-153) <0 0 1> <1 1 0> 0.114 174.8
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.119 174.8
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.132 82.4
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.138 206.0
Ni (mp-23) <1 1 0> <1 0 0> 0.140 329.6
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.148 285.5
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.154 142.7
Au (mp-81) <1 1 1> <1 1 1> 0.155 214.1
Ni (mp-23) <1 0 0> <1 0 0> 0.158 206.0
Cu (mp-30) <1 0 0> <1 0 0> 0.163 206.0
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.165 174.8
WS2 (mp-224) <0 0 1> <1 1 0> 0.166 174.8
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.167 174.8
PbS (mp-21276) <1 0 0> <1 0 0> 0.168 329.6
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.171 214.1
CdS (mp-672) <0 0 1> <1 1 0> 0.189 233.1
NaCl (mp-22862) <1 0 0> <1 0 0> 0.194 164.8
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.194 164.8
CdS (mp-672) <1 1 1> <1 0 0> 0.204 206.0
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.244 329.6
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.246 329.6
GaP (mp-2490) <1 1 0> <1 1 0> 0.252 174.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
158 96 96 0 0 0
96 158 96 0 0 0
96 96 158 0 0 0
0 0 0 71 0 0
0 0 0 0 71 0
0 0 0 0 0 71
Compliance Tensor Sij (10-12Pa-1)
11.8 -4.5 -4.5 0 0 0
-4.5 11.8 -4.5 0 0 0
-4.5 -4.5 11.8 0 0 0
0 0 0 14 0 0
0 0 0 0 14 0
0 0 0 0 0 14
Shear Modulus GV
55 GPa
Bulk Modulus KV
117 GPa
Shear Modulus GR
47 GPa
Bulk Modulus KR
117 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
117 GPa
Elastic Anisotropy
0.90
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TmSnRh2 (mp-865252) 0.0030 0.000 3
MnGaRu2 (mp-865140) 0.0029 0.065 3
TiAlOs2 (mp-865442) 0.0030 0.000 3
Be2CuIr (mp-867273) 0.0030 0.000 3
ScMnRh2 (mp-867850) 0.0026 0.000 3
LiMgSnPd (mp-7555) 0.0047 0.000 4
LiMgSnAu (mp-7554) 0.0047 0.088 4
LiMgSbPt (mp-571584) 0.0047 0.086 4
LiMgSbPd (mp-10179) 0.0047 0.096 4
LiMgSnPt (mp-11806) 0.0047 0.000 4
MnS (mp-850100) 0.0047 0.501 2
MgRe3 (mp-977283) 0.0047 0.269 2
NaEr3 (mp-976405) 0.0041 0.318 2
PmAg3 (mp-862878) 0.0027 0.000 2
RbS (mp-1057750) 0.0046 0.494 2
Br (mp-673171) 0.0047 0.630 1
Ti (mp-73) 0.0047 0.112 1
I (mp-684663) 0.0047 0.469 1
Cr (mp-90) 0.0047 0.000 1
Bi (mp-568610) 0.0047 0.136 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv In_d Cu_pv
Final Energy/Atom
-5.0956 eV
Corrected Energy
-20.3824 eV
Uncorrected energy = -20.3824 eV Corrected energy = -20.3824 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 103026
Submitted by
User remarks:
  • Copper indium zirconium (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)