Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.427 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 302.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 302.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 241.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 97.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 317.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 219.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 122.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 146.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 241.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 260.7 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 201.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 122.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 268.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 161.1 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 260.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 195.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 97.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 317.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 241.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 170.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 122.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 146.5 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 100.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 181.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 219.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 241.6 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 100.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 181.3 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 201.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 170.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 73.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 341.8 |
BN (mp-984) | <0 0 1> | <0 1 1> | 65.2 |
BN (mp-984) | <1 0 0> | <0 1 1> | 195.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 146.5 |
BN (mp-984) | <1 1 0> | <0 1 1> | 65.2 |
BN (mp-984) | <1 1 1> | <0 1 1> | 65.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 302.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 60.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 161.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 130.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 195.5 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 366.2 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 302.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 244.1 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 325.9 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 302.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 73.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 293.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 195.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrCa2In2Ge (mp-619206) | 0.4320 | 0.110 | 4 |
BaAu (mp-570775) | 0.2535 | 0.000 | 2 |
SrAu (mp-30420) | 0.2420 | 0.000 | 2 |
SrPd (mp-999143) | 0.2423 | 0.000 | 2 |
CeNi (mp-21188) | 0.2458 | 0.000 | 2 |
TbNi (mp-672240) | 0.2489 | 0.012 | 2 |
Zr2CoP (mp-29152) | 0.5043 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.4895 | 0.000 | 3 |
Hf2NiP (mp-5918) | 0.5344 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.1883 | 0.017 | 3 |
Zr2NiP (mp-29153) | 0.5761 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points9 |
U Values-- |
PseudopotentialsVASP PAW: Th Ni_pv |
Final Energy/Atom-7.0213 eV |
Corrected Energy-112.3412 eV
-112.3412 eV = -112.3412 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)