Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.905 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiGaSiO4 + SiO2 |
Band Gap4.310 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 243.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 185.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 193.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 200.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 139.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 200.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 139.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 144.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 243.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 243.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 267.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 193.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 289.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 144.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 338.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 289.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 169.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 162.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 338.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 144.9 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 338.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 243.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 231.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 162.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 338.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 338.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 338.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.9 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 224.4 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 254.1 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 338.1 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 267.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 144.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 338.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 241.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 193.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 202.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 243.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 241.5 |
BN (mp-984) | <1 0 1> | <0 1 1> | 200.9 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 267.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 289.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 231.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 338.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 96.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 139.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 338.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 289.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCr(SiO3)2 (mvc-6906) | 0.4179 | 0.057 | 4 |
LiCr(SiO3)2 (mp-510529) | 0.2639 | 0.003 | 4 |
LiFe(SiO3)2 (mp-19061) | 0.0883 | 0.001 | 4 |
LiSc(SiO3)2 (mp-6099) | 0.2764 | 0.001 | 4 |
LiV(SiO3)2 (mp-640515) | 0.2785 | 0.000 | 4 |
MgSiO3 (mp-1020125) | 0.5330 | 0.010 | 3 |
MgSiO3 (mp-1020361) | 0.4250 | 0.009 | 3 |
MnSiO3 (mp-19528) | 0.5785 | 0.003 | 3 |
FeSiO3 (mp-630331) | 0.5381 | 0.012 | 3 |
MgSiO3 (mp-1020117) | 0.5043 | 0.010 | 3 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.5147 | 0.003 | 5 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.5713 | 0.010 | 5 |
Li8NbNi3(PO4)6 (mp-765344) | 0.5478 | 0.106 | 5 |
Li8Fe3Sn(PO4)6 (mp-775125) | 0.5708 | 0.087 | 5 |
Li7FeCo3(PO4)6 (mp-780179) | 0.5582 | 0.085 | 5 |
Li4Mn2Fe3P6WO24 (mp-770860) | 0.6110 | 0.082 | 6 |
Li4Mn2Fe3Sb(PO4)6 (mp-776752) | 0.6097 | 0.083 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6102 | 0.073 | 6 |
Li4TiMn2Ni3(PO4)6 (mp-776756) | 0.6047 | 0.071 | 6 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.6156 | 0.100 | 6 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.6585 | 0.000 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points24 |
U Values-- |
PseudopotentialsVASP PAW: Li_sv O Si Ga_d |
Final Energy/Atom-7.0237 eV |
Corrected Energy-297.8021 eV
-297.8021 eV = -280.9471 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)