Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.203 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiC |
Band Gap2.054 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 24.9 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 124.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 8.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 124.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 141.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 282.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 216.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 74.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 166.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 83.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 157.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 324.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 58.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 166.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 149.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 108.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 157.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 266.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 315.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 157.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 83.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 232.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 266.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 299.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 216.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 216.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 266.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 266.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 166.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 290.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 58.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 224.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 324.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 58.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 207.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 290.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 157.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 166.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 166.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 108.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 290.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Si3NiP4 (mp-8311) | 0.1962 | 0.000 | 3 |
Cu2SiTe3 (mp-675120) | 0.1918 | 0.001 | 3 |
Li3SbS4 (mp-760415) | 0.1891 | 0.005 | 3 |
CrCd3Te4 (mp-1079533) | 0.1947 | 0.115 | 3 |
Cu3AsS4 (mp-3345) | 0.1940 | 0.000 | 3 |
ZnCu2GeS4 (mp-6408) | 0.1725 | 0.000 | 4 |
CoCu2SiS4 (mp-11769) | 0.1841 | 0.065 | 4 |
ZnCu2SiTe4 (mp-1078498) | 0.1843 | 0.000 | 4 |
LiIn2CuSe4 (mp-1079491) | 0.1823 | 0.004 | 4 |
ZnCu2SnS4 (mp-1079541) | 0.1804 | 0.000 | 4 |
SiC (mp-570985) | 0.0138 | 0.000 | 2 |
ZnS (mp-18377) | 0.0156 | 0.012 | 2 |
SiC (mp-567551) | 0.0141 | 0.000 | 2 |
SiC (mp-570804) | 0.0148 | 0.032 | 2 |
SiC (mp-11713) | 0.0146 | 0.003 | 2 |
C (mp-611448) | 0.0354 | 0.143 | 1 |
C (mp-616440) | 0.0432 | 0.141 | 1 |
C (mp-569517) | 0.0347 | 0.145 | 1 |
C (mp-569567) | 0.0346 | 0.144 | 1 |
Ge (mp-1091415) | 0.0569 | 0.008 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si C |
Final Energy/Atom-7.5277 eV |
Corrected Energy-165.6085 eV
-165.6085 eV = -165.6085 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)