Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.676 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH3N + H5NO + N2 |
Band Gap3.883 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3121 [152] |
HallP 31 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 270.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 156.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 271.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 146.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 376.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 271.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 270.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 209.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 20.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 334.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 260.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 167.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 208.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 270.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 376.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 260.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 208.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 62.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 230.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 271.9 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 337.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 260.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 208.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 83.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 313.7 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 180.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 188.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 208.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 146.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 104.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 146.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 271.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 146.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 146.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 146.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 188.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 156.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 271.9 |
BN (mp-984) | <1 1 1> | <1 1 0> | 270.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 271.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 62.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 188.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 52.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 313.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 209.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgH8O5 (mp-769295) | 0.6154 | 0.079 | 3 |
H5NO (mp-625924) | 0.4916 | 0.004 | 3 |
LiH3O2 (mp-27281) | 0.6118 | 0.002 | 3 |
H5NO (mp-625927) | 0.6307 | 0.029 | 3 |
NaH3O2 (mp-625391) | 0.6552 | 0.003 | 3 |
CaH8(ClO2)2 (mp-721047) | 0.6592 | 0.018 | 4 |
HgH2NCl (mp-643754) | 0.6165 | 0.101 | 4 |
LiH2IO (mp-643708) | 0.6483 | 0.001 | 4 |
NaH4IO2 (mp-696512) | 0.6458 | 0.014 | 4 |
KH2I3O (mp-696649) | 0.6587 | 0.005 | 4 |
H2O (mp-557082) | 0.7448 | 0.034 | 2 |
H2O (mp-558226) | 0.7297 | 0.033 | 2 |
H2O (mp-697085) | 0.6170 | 0.064 | 2 |
FeCl3 (mp-676241) | 0.7042 | 0.024 | 2 |
H2O (mp-32959) | 0.6157 | 0.067 | 2 |
NaH4CNO2 (mp-632685) | 0.6281 | 0.203 | 5 |
NaH4CNO2 (mp-706281) | 0.6901 | 0.160 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H N O |
Final Energy/Atom-5.0747 eV |
Corrected Energy-139.1232 eV
-139.1232 eV = -137.0163 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)