material

Zn(HO)2

ID:

mp-625487

DOI:

10.17188/1278397


Tags: Zinc hydroxide - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-1.472 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.084 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.02 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zn(HO)2
Band Gap
2.426 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge (mp-32) <1 1 1> <0 0 1> 0.000 172.7
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.001 76.0
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.002 227.2
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.006 145.4
GaAs (mp-2534) <1 1 1> <0 0 1> 0.006 172.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.007 227.2
Ni (mp-23) <1 1 1> <0 0 1> 0.007 63.6
SiC (mp-7631) <1 0 0> <1 0 1> 0.008 189.4
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.008 146.3
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.008 117.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.009 281.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.010 227.2
KP(HO2)2 (mp-23959) <1 0 1> <1 0 1> 0.011 137.8
SiC (mp-11714) <1 0 0> <1 0 1> 0.012 189.4
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.013 53.8
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.014 43.9
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.015 327.2
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.015 172.7
InAs (mp-20305) <1 1 0> <1 0 0> 0.015 160.9
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.016 160.9
C (mp-66) <1 1 0> <1 0 0> 0.018 160.9
SiC (mp-8062) <1 1 0> <1 0 0> 0.019 160.9
KCl (mp-23193) <1 0 0> <1 1 0> 0.021 202.7
SiC (mp-7631) <1 1 0> <1 0 0> 0.021 160.9
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 0 0> 0.021 160.9
NdGaO3 (mp-3196) <1 1 1> <1 1 0> 0.022 202.7
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.022 117.0
Te2W (mp-22693) <1 1 0> <1 0 1> 0.023 223.9
GaN (mp-804) <1 0 0> <1 0 0> 0.023 102.4
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.025 86.1
SiC (mp-11714) <1 0 1> <1 0 1> 0.027 258.3
GaTe (mp-542812) <1 0 1> <1 0 1> 0.028 292.8
AlN (mp-661) <0 0 1> <0 0 1> 0.029 109.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.029 219.4
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.029 277.9
ZrO2 (mp-2858) <0 0 1> <1 0 1> 0.030 223.9
CsI (mp-614603) <1 1 0> <1 0 0> 0.031 87.8
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.031 228.0
SiC (mp-7631) <0 0 1> <0 0 1> 0.032 109.0
CdSe (mp-2691) <1 1 0> <1 0 0> 0.033 160.9
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.034 117.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.035 109.0
Te2Mo (mp-602) <1 0 1> <1 0 1> 0.036 223.9
LaAlO3 (mp-2920) <1 1 0> <1 0 0> 0.036 248.7
MgAl2O4 (mp-3536) <1 1 0> <1 0 0> 0.037 277.9
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.038 126.7
LaF3 (mp-905) <1 1 0> <1 1 1> 0.038 188.4
Au (mp-81) <1 1 0> <1 0 1> 0.039 223.9
GaSb (mp-1156) <1 1 0> <1 0 0> 0.039 160.9
KP(HO2)2 (mp-23959) <1 1 0> <1 0 1> 0.040 137.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
136 64 13 5 0 0
64 136 13 -5 -0 0
13 13 45 0 -0 0
5 -5 0 19 0 -0
0 -0 -0 0 19 5
0 0 0 -0 5 36
Compliance Tensor Sij (10-12Pa-1)
9.7 -4.5 -1.5 -3.5 0 0
-4.5 9.7 -1.5 3.5 0 0
-1.5 -1.5 23.3 0 0 0
-3.5 3.5 0 54.4 0 0
0 0 0 0 54.4 -6.9
0 0 0 0 -6.9 28.6
Shear Modulus GV
30 GPa
Bulk Modulus KV
55 GPa
Shear Modulus GR
24 GPa
Bulk Modulus KR
36 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
46 GPa
Elastic Anisotropy
1.64
Poisson's Ratio
0.25

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
123
U Values
--
Pseudopotentials
VASP PAW: Zn H O
Final Energy/Atom
-4.7151 eV
Corrected Energy
-24.9803 eV
-24.9803 eV = -23.5757 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 20285

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)