Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.233 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH9BrO4 |
Band Gap4.041 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 247.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 264.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 266.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 317.4 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 293.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 264.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 211.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 247.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 88.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 264.5 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 206.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 293.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 317.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 317.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 247.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 247.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 266.3 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 222.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 264.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 177.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 211.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 317.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 266.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 293.7 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 293.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 158.7 |
BN (mp-984) | <1 1 0> | <1 0 0> | 266.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 140.5 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 247.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 317.4 |
BN (mp-984) | <0 0 1> | <0 1 0> | 264.5 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 140.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 140.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 211.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 247.2 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 1 0> | 264.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 211.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 -1> | 293.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 247.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 317.4 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 293.7 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 195.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 317.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 264.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 88.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 317.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 211.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 264.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 164.8 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 211.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H7BrO3 (mp-625560) | 0.4240 | 0.016 | 3 |
H7BrO3 (mp-625555) | 0.3989 | 0.034 | 3 |
H9BrO4 (mp-625614) | 0.4402 | 0.018 | 3 |
H9BrO4 (mp-625604) | 0.3931 | 0.028 | 3 |
H9BrO4 (mp-625653) | 0.3021 | 0.026 | 3 |
NaH5S2O9 (mp-733973) | 0.6551 | 0.555 | 4 |
TiH12N3F7 (mp-684736) | 0.7260 | 0.503 | 4 |
TeH12(Cl2O3)2 (mp-707765) | 0.6363 | 0.017 | 4 |
CuH10SO9 (mp-605120) | 0.7391 | 0.797 | 4 |
MnH6SO6 (mp-735543) | 0.7267 | 0.260 | 4 |
CoH22S2N5O9 (mp-735625) | 0.7295 | 0.539 | 5 |
H9CSO7F3 (mp-720860) | 0.6251 | 0.111 | 5 |
P2H17C4NO8 (mp-559679) | 0.7389 | 0.096 | 5 |
SiH12N2(O2F3)2 (mp-743965) | 0.7022 | 0.525 | 5 |
TeH14C3S3(N3F2)2 (mp-849783) | 0.7457 | 0.097 | 6 |
CuH9CSN4Cl3O (mp-706528) | 0.7408 | 0.436 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H Br O |
Final Energy/Atom-4.6453 eV |
Corrected Energy-273.2656 eV
Uncorrected energy = -260.1376 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-0.534 eV/atom x 4.0 atoms) = -2.1360 eV
Corrected energy = -273.2656 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)