Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.836 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.242 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg(HO)2 |
Band Gap4.137 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 93.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 107.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 124.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 314.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 124.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 233.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 166.5 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 124.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 295.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 155.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 55.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 169.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 159.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 99.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 202.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 240.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 342.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 186.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 140.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 258.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 124.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 279.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 55.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 332.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 221.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 314.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 57.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 323.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 186.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 295.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 189.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 99.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 171.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 201.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 148.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 309.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 179.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 199.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.28636 | 0.05840 |
0.05840 | -0.05840 | 0.00000 | -0.28636 | 0.00000 | 0.00000 |
-0.21784 | -0.21784 | -0.37362 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.48425 C/m2 |
Crystallographic Direction vmax |
---|
-0.00000 |
0.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.63 | 0.00 | 0.00 |
0.00 | 2.63 | 0.00 |
0.00 | 0.00 | 2.37 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.44 | 0.00 | -0.00 |
0.00 | 10.44 | 0.00 |
-0.00 | 0.00 | 4.50 |
Polycrystalline dielectric constant
εpoly∞
2.54
|
Polycrystalline dielectric constant
εpoly
8.46
|
Refractive Index n1.59 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv H O |
Final Energy/Atom-5.1495 eV |
Corrected Energy-27.1215 eV
Uncorrected energy = -25.7475 eV
Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV
Corrected energy = -27.1215 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)