Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.622 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.772 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 1 0> | <1 0 0> | 240.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 320.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 138.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 113.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 240.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 113.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 240.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 240.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 113.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 320.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 240.0 |
Al (mp-134) | <1 1 0> | <1 1 0> | 138.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 113.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 240.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 240.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 320.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 320.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 138.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 320.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 113.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 138.9 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 240.0 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 138.6 |
C (mp-48) | <1 1 1> | <1 0 0> | 240.0 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 320.0 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 113.6 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 113.6 |
ZnO (mp-2133) | <1 1 0> | <1 0 0> | 240.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
In(HO)3 (mp-626411) | 0.0243 | 0.000 | 3 |
Sc(HO)3 (mp-626194) | 0.1308 | 0.015 | 3 |
Sc(HO)3 (mp-626193) | 0.1317 | 0.016 | 3 |
Lu(HO)3 (mp-625468) | 0.1298 | 0.000 | 3 |
Lu(HO)3 (mp-625392) | 0.1670 | 0.001 | 3 |
Sr2Sn(HO)8 (mp-766178) | 0.6154 | 0.032 | 4 |
Na2Hf(HO)6 (mp-643896) | 0.5739 | 0.018 | 4 |
TcSb(OF4)2 (mp-555059) | 0.5774 | 0.000 | 4 |
AsS(IF3)2 (mp-557628) | 0.6351 | 0.000 | 4 |
SbMoOF9 (mp-567264) | 0.5891 | 0.000 | 4 |
TaF5 (mp-561197) | 0.6057 | 0.000 | 2 |
UF6 (mp-672341) | 0.5290 | 0.004 | 2 |
MoF5 (mp-555649) | 0.5660 | 0.078 | 2 |
NbF5 (mp-18687) | 0.5939 | 0.000 | 2 |
MoF5 (mp-608126) | 0.5688 | 0.078 | 2 |
Rb2NaCr(CN)6 (mp-17509) | 0.7030 | 0.203 | 5 |
LiAl2H6ClO6 (mp-643655) | 0.6136 | 0.000 | 5 |
K3ReC4(N2O)2 (mp-540813) | 0.6987 | 0.105 | 5 |
Rb2NaMn(CN)6 (mp-505659) | 0.7171 | 0.171 | 5 |
LiAl2H6BrO6 (mp-1097038) | 0.6218 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d H O |
Final Energy/Atom-5.2232 eV |
Corrected Energy-154.6772 eV
-154.6772 eV = -146.2497 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)