Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.833 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr(HO)2 + H2O |
Band Gap4.400 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 200.0 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 259.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 200.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 133.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 155.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 155.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 244.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 148.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 160.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 128.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 146.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 244.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 299.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 200.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 148.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 111.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 88.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 128.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 259.3 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 1> | 277.6 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 251.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 176.3 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 244.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 214.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 296.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 222.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 111.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 128.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 355.6 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 264.4 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 264.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 146.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 117.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 311.2 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 185.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 288.9 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 222.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 200.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 200.0 |
LiF (mp-1138) | <1 0 0> | <1 -1 1> | 166.6 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 117.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 311.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 214.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 106.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 176.0 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 185.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 200.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 66.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 259.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.19295 | 0.36093 | 0.10172 | -0.03667 | 0.05005 | 0.35711 |
0.01124 | 0.37047 | 0.13800 | -0.12137 | 0.08608 | 0.08761 |
0.18758 | -0.39059 | 0.29984 | 0.16211 | -0.04998 | 0.07759 |
Piezoelectric Modulus ‖eij‖max0.71741 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
1.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.67 | 0.03 | -0.00 |
0.03 | 2.61 | -0.02 |
-0.00 | -0.02 | 2.48 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.59 | 1.28 | -0.59 |
1.28 | 8.90 | -0.97 |
-0.59 | -0.97 | 8.27 |
Polycrystalline dielectric constant
εpoly∞
2.58
|
Polycrystalline dielectric constant
εpoly
8.92
|
Refractive Index n1.61 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrH4O3 (mp-626755) | 0.5774 | 0.037 | 3 |
BaH4O3 (mp-626735) | 0.5613 | 0.010 | 3 |
BaH4O3 (mp-626726) | 0.6162 | 0.007 | 3 |
Sr(H2O3)2 (mp-625871) | 0.5368 | 0.112 | 3 |
H4N2O3 (mp-625664) | 0.5888 | 0.979 | 3 |
CaH8(ClO2)2 (mp-721047) | 0.7020 | 0.018 | 4 |
MoH2Cl2O3 (mp-743614) | 0.7326 | 0.029 | 4 |
KHSeO3 (mp-24433) | 0.6668 | 0.015 | 4 |
KH2I3O (mp-696649) | 0.6899 | 0.005 | 4 |
HgH4C4(Br2N)2 (mp-709400) | 0.7038 | 0.991 | 5 |
NaH4CNO2 (mp-632685) | 0.6123 | 0.203 | 5 |
HgH4C4(NCl2)2 (mp-736259) | 0.6699 | 0.956 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv H O |
Final Energy/Atom-5.2566 eV |
Corrected Energy-88.2284 eV
Uncorrected energy = -84.1064 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -88.2284 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)