Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.300 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr3AgO8 + Ag3O4 + AgO |
Band Gap1.350 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <1 -1 0> | 131.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 246.2 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 0> | 327.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 319.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 273.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 281.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 252.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 136.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 302.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 273.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 281.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 273.5 |
ZnSe (mp-1190) | <1 1 1> | <1 -1 0> | 327.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 161.1 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 211.0 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 317.0 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 211.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 319.1 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 131.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 302.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 322.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 190.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 182.4 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 214.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 182.4 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 268.4 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 268.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 -1 0> | 327.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 211.0 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 0> | 131.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 319.1 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 161.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 252.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 252.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 -1> | 317.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 -1> | 317.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 -1> | 190.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 285.4 |
CdTe (mp-406) | <1 0 0> | <1 -1 0> | 131.2 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 302.7 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 268.4 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 237.8 |
LiTaO3 (mp-3666) | <0 0 1> | <1 -1 0> | 327.9 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 1> | 246.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 237.8 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 273.1 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 246.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 -1> | 190.2 |
TiO2 (mp-2657) | <1 0 1> | <1 -1 1> | 180.8 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 136.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2S2O7 (mp-31269) | 0.5570 | 0.000 | 3 |
Cd2P2O7 (mp-27686) | 0.5194 | 0.000 | 3 |
Sn2P2O7 (mp-753979) | 0.5610 | 0.049 | 3 |
Na2Cr2O7 (mp-704459) | 0.5174 | 0.000 | 3 |
Ge2BiO6 (mvc-8139) | 0.5617 | 0.083 | 3 |
MgTiP2O7 (mvc-5367) | 0.5236 | 0.238 | 4 |
LiSbP2O7 (mp-759493) | 0.4897 | 0.094 | 4 |
Na2CaP2O7 (mp-561260) | 0.5588 | 0.000 | 4 |
LiSbP2O7 (mp-673073) | 0.5383 | 0.038 | 4 |
LiBiP2O7 (mp-672979) | 0.5262 | 0.022 | 4 |
KNaZnP2O7 (mp-554157) | 0.5367 | 0.000 | 5 |
LiVSO4F3 (mp-768092) | 0.7035 | 0.057 | 5 |
BaNaNd(GeO3)3 (mp-14353) | 0.6245 | 0.006 | 5 |
BaNaEu(SiO3)3 (mp-1019735) | 0.6396 | 0.000 | 5 |
BaNaNd(SiO3)3 (mp-13791) | 0.6557 | 0.002 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv Ag O |
Final Energy/Atom-5.9057 eV |
Corrected Energy-147.8092 eV
-147.8092 eV = -129.9251 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)