Final Magnetic Moment5.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.794 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.988 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 124.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 152.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 249.1 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 124.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 88.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 152.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 249.1 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 88.1 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 124.6 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 249.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 88.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 176.2 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 124.6 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 124.6 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 264.2 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 264.2 |
Si (mp-149) | <1 1 0> | <1 1 0> | 124.6 |
Si (mp-149) | <1 1 1> | <1 1 1> | 152.6 |
C (mp-48) | <1 0 0> | <1 1 0> | 249.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 1 0> | 249.1 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 249.1 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 88.1 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 88.1 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 264.2 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 124.6 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 124.6 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 264.2 |
CaF2 (mp-2741) | <1 1 1> | <1 0 0> | 264.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 124.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 249.1 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 152.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 249.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 264.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 88.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 249.1 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 264.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 176.2 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 88.1 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 152.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 88.1 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 152.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K3ReH6 (mp-690789) | 0.1017 | 0.183 | 3 |
Li6Br3N (mp-27508) | 0.0539 | 0.070 | 3 |
TiTl3F6 (mp-15635) | 0.0154 | 0.095 | 3 |
V(NF2)3 (mp-1078732) | 0.0057 | 1.442 | 3 |
K3AlF6 (mp-1095079) | 0.0062 | 0.000 | 3 |
Cs2NaGaH6 (mp-989594) | 0.0119 | 0.072 | 4 |
Rb2TlGaF6 (mp-989565) | 0.0026 | 0.000 | 4 |
Cs2TlVF6 (mp-637063) | 0.0255 | 0.000 | 4 |
Cs2KCoF6 (mp-567007) | 0.0345 | 0.000 | 4 |
Cs2TlVF6 (mp-557533) | 0.0207 | 0.000 | 4 |
Cs2KZrOF5 (mp-40143) | 0.3674 | 0.000 | 5 |
KRb2ZrOF5 (mp-39542) | 0.3951 | 0.020 | 5 |
KZrTl2OF5 (mp-40204) | 0.4525 | 0.058 | 5 |
Cs2RbZrOF5 (mp-42022) | 0.3140 | 0.006 | 5 |
Cs2ZrTlOF5 (mp-42227) | 0.3858 | 0.017 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.7191 | 0.057 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Cs_sv Tl_d Fe_pv F |
Final Energy/Atom-4.6358 eV |
Corrected Energy-49.0906 eV
-49.0906 eV = -46.3576 eV (uncorrected energy) - 2.7330 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)