Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.796 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.506 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnCO3 + CO2 + MnBr2 + C |
Band Gap2.764 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 101.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 219.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 70.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 219.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 282.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 154.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 282.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 146.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 135.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 212.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 282.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 219.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 282.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 282.8 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 219.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 282.8 |
BN (mp-984) | <0 0 1> | <1 0 1> | 153.1 |
BN (mp-984) | <1 0 0> | <0 1 0> | 292.0 |
Al (mp-134) | <1 0 0> | <0 1 0> | 146.0 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 203.3 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 153.1 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 153.1 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 292.0 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 154.2 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 73.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 219.0 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 292.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 292.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 219.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 282.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 282.8 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 101.6 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 73.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 282.8 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 212.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 146.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 292.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 1> | 153.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 73.0 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 212.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 282.8 |
WSe2 (mp-1821) | <0 0 1> | <1 0 1> | 153.1 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 135.8 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 212.1 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 219.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 219.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 292.0 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 212.1 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 292.0 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 282.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tc(CO)5 (mp-680571) | 0.5583 | 0.211 | 3 |
MoH4O5 (mp-625711) | 0.7430 | 0.204 | 3 |
Re(CO)5 (mp-540820) | 0.5905 | 0.229 | 3 |
MnC5ClO5 (mp-623924) | 0.2509 | 0.518 | 4 |
ReC5IO5 (mp-616468) | 0.3816 | 0.173 | 4 |
ReC5BrO5 (mp-620054) | 0.2448 | 0.154 | 4 |
ReC5ClO5 (mp-648163) | 0.3790 | 0.177 | 4 |
Re2Pt(CO)12 (mp-614325) | 0.4429 | 0.242 | 4 |
Mn2InC10BrO10 (mp-683668) | 0.6727 | 0.566 | 5 |
Mn2SnC10(BrO5)2 (mp-637929) | 0.6248 | 0.532 | 5 |
Mn2SnC10(ClO5)2 (mp-637617) | 0.6439 | 0.530 | 5 |
GeW2C10(BrO5)2 (mp-704542) | 0.5073 | 0.488 | 5 |
Mn2SnC10BrO10 (mp-705194) | 0.6355 | 0.584 | 5 |
Fe3PWC15BrO15 (mp-704755) | 0.7407 | 0.705 | 6 |
K3HRhC5N5O (mp-697108) | 0.7118 | 0.101 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv C Br O |
Final Energy/Atom-7.1694 eV |
Corrected Energy-364.9008 eV
-364.9008 eV = -344.1316 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)