Final Magnetic Moment0.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.955 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa + NbTc + Tc |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 328.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 262.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 196.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 241.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 80.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 232.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 232.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 328.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 160.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 232.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 131.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 196.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 139.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 241.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 139.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 262.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 328.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 278.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 241.1 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 196.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 262.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 324.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 232.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 232.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 241.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 232.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 232.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 196.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 262.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 232.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 328.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 46.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 232.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 139.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 92.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 328.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 65.6 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 80.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 232.0 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 196.8 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 232.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 185.6 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 196.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 232.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 196.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 160.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 278.3 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 262.4 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 232.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnGaRh2 (mp-977362) | 0.0000 | 0.000 | 3 |
Ba2BeGa (mp-631574) | 0.0000 | 0.584 | 3 |
Zn2NiIr (mp-971836) | 0.0000 | 0.008 | 3 |
Al2FeCo (mp-862691) | 0.0000 | 0.000 | 3 |
Be2PdRh (mp-866115) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0000 | 0.221 | 4 |
Sr3Yb (mp-981378) | 0.0000 | 0.033 | 2 |
Rb3Hg (mp-974990) | 0.0000 | 0.069 | 2 |
Ti3Al (mp-999027) | 0.0000 | 0.119 | 2 |
Cr3Fe (mp-1008282) | 0.0000 | 0.127 | 2 |
Ba3Np (mp-1076925) | 0.0000 | 0.681 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nb_pv Tc_pv |
Final Energy/Atom-7.2305 eV |
Corrected Energy-28.9222 eV
-28.9222 eV = -28.9222 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)