Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.897 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.103 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKHg2 + B |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 159.7 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 276.6 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 225.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 266.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 266.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 225.8 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 276.6 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 276.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 266.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 225.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 266.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 225.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 150.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 212.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 225.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 276.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 266.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 266.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 225.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 276.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 266.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 212.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 150.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 212.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 225.8 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 225.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 212.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 319.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 212.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 266.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 225.8 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 225.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 75.3 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 92.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 276.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 266.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 159.7 |
BN (mp-984) | <1 1 0> | <1 1 1> | 276.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 212.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 225.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 266.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 266.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 266.1 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 212.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 92.2 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 75.3 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 92.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlVFeCo (mp-1008530) | 0.0000 | 0.028 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.027 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.025 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.009 | 4 |
Rb3Y (mp-974732) | 0.0000 | 0.617 | 2 |
Na3Al (mp-974270) | 0.0000 | 0.173 | 2 |
Yb3Mg (mp-980034) | 0.0000 | 0.048 | 2 |
Nb3Cr (mp-999439) | 0.0000 | 0.123 | 2 |
NbCr3 (mp-999390) | 0.0000 | 0.118 | 2 |
YErTl2 (mp-981548) | 0.0000 | 0.004 | 3 |
BeW2Cl (mp-631535) | 0.0000 | 1.620 | 3 |
CrInNi2 (mp-1007991) | 0.0000 | 0.329 | 3 |
CrCo2Bi (mp-1018080) | 0.0000 | 0.399 | 3 |
CrCo2Si (mp-1008224) | 0.0000 | 0.038 | 3 |
Ge (mp-998883) | 0.0000 | 0.346 | 1 |
Ni (mp-1008728) | 0.0000 | 0.097 | 1 |
Si (mp-1014212) | 0.0000 | 0.541 | 1 |
Cu (mp-998890) | 0.0000 | 0.034 | 1 |
Al (mp-998860) | 0.0000 | 0.095 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: K_sv Hg B |
Final Energy/Atom-1.1995 eV |
Corrected Energy-4.7982 eV
-4.7982 eV = -4.7982 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)