Final Magnetic Moment0.101 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.871 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.613 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBe2W + W + BeCl2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 287.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 62.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 215.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 152.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 108.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 144.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 251.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 323.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 287.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 144.0 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 62.3 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 311.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 187.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 179.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 108.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 179.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 36.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 50.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 203.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 215.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 187.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 287.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 101.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 36.0 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 50.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 251.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 251.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 287.9 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 323.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 179.9 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 305.4 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 187.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 36.0 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 50.9 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 62.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 144.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 36.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 50.9 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 62.3 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 179.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 1 0> | 305.4 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 287.9 |
SiC (mp-11714) | <1 0 1> | <1 1 0> | 254.5 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 359.9 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 0> | 152.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 36.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 179.9 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 152.7 |
Ga2O3 (mp-886) | <1 1 1> | <1 1 0> | 254.5 |
Si (mp-149) | <1 0 0> | <1 0 0> | 144.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
260 | 181 | 181 | 0 | 0 | 0 |
181 | 260 | 181 | 0 | 0 | 0 |
181 | 181 | 260 | 0 | 0 | 0 |
0 | 0 | 0 | 37 | 0 | 0 |
0 | 0 | 0 | 0 | 37 | 0 |
0 | 0 | 0 | 0 | 0 | 37 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.9 | -3.6 | -3.6 | 0 | 0 | 0 |
-3.6 | 8.9 | -3.6 | 0 | 0 | 0 |
-3.6 | -3.6 | 8.9 | 0 | 0 | 0 |
0 | 0 | 0 | 26.7 | 0 | 0 |
0 | 0 | 0 | 0 | 26.7 | 0 |
0 | 0 | 0 | 0 | 0 | 26.7 |
Shear Modulus GV38 GPa |
Bulk Modulus KV207 GPa |
Shear Modulus GR38 GPa |
Bulk Modulus KR207 GPa |
Shear Modulus GVRH38 GPa |
Bulk Modulus KVRH207 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.41 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2ZnPb (mp-977424) | 0.0000 | 0.000 | 3 |
ReRuCl2 (mp-631417) | 0.0000 | 1.819 | 3 |
SrTa2Mn (mp-631358) | 0.0000 | 1.217 | 3 |
LiTaW2 (mp-631330) | 0.0000 | 0.618 | 3 |
Ac2GaCu (mp-862683) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
Sn3B (mp-978917) | 0.0000 | 0.937 | 2 |
Rb3Pm (mp-983446) | 0.0000 | 0.624 | 2 |
Rb3Nd (mp-974850) | 0.0000 | 0.613 | 2 |
Ti3Si (mp-998986) | 0.0000 | 0.194 | 2 |
Cu3Sn (mp-838) | 0.0000 | 0.074 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Be_sv W_pv Cl |
Final Energy/Atom-6.8560 eV |
Corrected Energy-27.4239 eV
-27.4239 eV = -27.4239 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)