Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.903 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.921 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSi + SiB3 + Au |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 220.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 317.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 44.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 55.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 158.9 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 158.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 254.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 349.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 89.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 314.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 220.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 222.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 134.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 95.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 158.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 179.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 220.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 190.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 254.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 31.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 89.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 127.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 269.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 44.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 158.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 63.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 158.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 222.5 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 314.6 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 165.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 31.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 44.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 55.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 31.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 44.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 314.6 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 220.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 254.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 158.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 222.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 254.2 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 220.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 254.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 286.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 158.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 269.7 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 179.8 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 220.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 165.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 95.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
111 | 152 | 152 | 0 | 0 | 0 |
152 | 111 | 152 | 0 | 0 | 0 |
152 | 152 | 111 | 0 | 0 | 0 |
0 | 0 | 0 | -252 | 0 | 0 |
0 | 0 | 0 | 0 | -252 | 0 |
0 | 0 | 0 | 0 | 0 | -252 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-15.7 | 9 | 9 | 0 | 0 | 0 |
9 | -15.7 | 9 | 0 | 0 | 0 |
9 | 9 | -15.7 | 0 | 0 | 0 |
0 | 0 | 0 | -4 | 0 | 0 |
0 | 0 | 0 | 0 | -4 | 0 |
0 | 0 | 0 | 0 | 0 | -4 |
Shear Modulus GV-159 GPa |
Bulk Modulus KV138 GPa |
Shear Modulus GR-45 GPa |
Bulk Modulus KR138 GPa |
Shear Modulus GVRH-102 GPa |
Bulk Modulus KVRH138 GPa |
Elastic Anisotropy12.67 |
Poisson's Ratio0.99 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BeGeB (mp-631541) | 0.0000 | 0.764 | 3 |
ZrCrFe (mp-631429) | 0.0000 | 0.889 | 3 |
FeNiMo (mp-631256) | 0.0000 | 0.604 | 3 |
InSiIr (mp-631255) | 0.0000 | 1.148 | 3 |
MnCoSe (mp-1008873) | 0.0000 | 0.178 | 3 |
YbH2 (mp-634751) | 0.0000 | 0.059 | 2 |
ErH2 (mp-24192) | 0.0000 | 0.000 | 2 |
Al2Pt (mp-1502) | 0.0000 | 0.000 | 2 |
Ti2Si (mp-1008689) | 0.0000 | 0.968 | 2 |
EuF2 (mp-561850) | 0.0000 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si B Au |
Final Energy/Atom-4.2229 eV |
Corrected Energy-12.6686 eV
-12.6686 eV = -12.6686 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)