Final Magnetic Moment0.139 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.704 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.722 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density15.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi + Os + BiAu2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 299.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 249.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 249.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 282.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 199.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 211.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 259.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 282.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 249.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 199.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 211.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 259.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 249.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 282.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 86.4 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 211.6 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 149.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 149.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 349.2 |
Al (mp-134) | <1 1 0> | <1 1 0> | 70.5 |
Al (mp-134) | <1 1 1> | <1 1 1> | 86.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 259.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 249.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 211.6 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 259.2 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 282.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 349.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 141.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 249.4 |
C (mp-66) | <1 1 1> | <1 0 0> | 349.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 282.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 282.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 172.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 211.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 199.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 211.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 141.1 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 249.4 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 349.2 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 249.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 349.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 70.5 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 86.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 282.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 149.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 149.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 211.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
76 | 122 | 122 | 0 | 0 | 0 |
122 | 76 | 122 | 0 | 0 | 0 |
122 | 122 | 76 | 0 | 0 | 0 |
0 | 0 | 0 | 25 | 0 | 0 |
0 | 0 | 0 | 0 | 25 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-13.5 | 8.3 | 8.3 | 0 | 0 | 0 |
8.3 | -13.5 | 8.3 | 0 | 0 | 0 |
8.3 | 8.3 | -13.5 | 0 | 0 | 0 |
0 | 0 | 0 | 39.4 | 0 | 0 |
0 | 0 | 0 | 0 | 39.4 | 0 |
0 | 0 | 0 | 0 | 0 | 39.4 |
Shear Modulus GV6 GPa |
Bulk Modulus KV107 GPa |
Shear Modulus GR160 GPa |
Bulk Modulus KR107 GPa |
Shear Modulus GVRH83 GPa |
Bulk Modulus KVRH107 GPa |
Elastic Anisotropy-4.81 |
Poisson's Ratio0.19 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaSiTc2 (mp-631504) | 0.0000 | 1.264 | 3 |
LaMgNb2 (mp-631336) | 0.0000 | 0.698 | 3 |
InP2Pb (mp-631312) | 0.0000 | 0.684 | 3 |
Lu2TcPd (mp-865413) | 0.0000 | 0.093 | 3 |
TaBeRu2 (mp-867114) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoAs (mp-998974) | 0.0000 | 0.134 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0000 | 0.212 | 4 |
K3Si (mp-973528) | 0.0000 | 0.333 | 2 |
SnTe3 (mp-978885) | 0.0000 | 0.325 | 2 |
NaCd3 (mp-865077) | 0.0000 | 0.000 | 2 |
Ti3Ga (mp-998988) | 0.0000 | 0.129 | 2 |
FeNi3 (mp-1007854) | 0.0000 | 0.108 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi Os_pv Au |
Final Energy/Atom-4.8662 eV |
Corrected Energy-19.4649 eV
-19.4649 eV = -19.4649 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)