Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.385 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.584 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa8Ga7 + Ba + Be |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 87.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 308.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 308.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 174.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 87.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 184.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 61.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 308.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 308.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 308.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 261.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 308.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 61.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 308.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 106.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 174.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 308.0 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 106.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 308.0 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 261.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 261.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 246.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 174.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 308.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 308.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 308.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 308.0 |
BN (mp-984) | <1 0 0> | <1 1 0> | 174.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 246.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 246.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 184.8 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 261.4 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 246.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 106.7 |
Al (mp-134) | <1 0 0> | <1 1 0> | 261.4 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 261.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 261.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 246.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 184.8 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 261.4 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 308.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 308.0 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 87.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 308.0 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 308.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 87.1 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 184.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 61.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 87.1 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 184.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnGaRh2 (mp-977362) | 0.0000 | 0.000 | 3 |
Zn2NiIr (mp-971836) | 0.0000 | 0.008 | 3 |
BaNbTc2 (mp-631491) | 0.0000 | 1.020 | 3 |
Be2PdRh (mp-866115) | 0.0000 | 0.000 | 3 |
Sc2MnSi (mp-999208) | 0.0000 | 0.266 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
Y3Sn (mp-1094256) | 0.0000 | 0.278 | 2 |
Rb3V (mp-974743) | 0.0000 | 0.925 | 2 |
Rb3Hg (mp-974990) | 0.0000 | 0.069 | 2 |
Cr3Fe (mp-1008282) | 0.0000 | 0.127 | 2 |
Ba3Np (mp-1076925) | 0.0000 | 0.681 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Be_sv Ga_d |
Final Energy/Atom-2.2663 eV |
Corrected Energy-9.0651 eV
-9.0651 eV = -9.0651 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)