Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.706 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.833 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRe + LaAg |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 228.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 323.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 258.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 194.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 274.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 194.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 64.7 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 79.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 228.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 194.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 228.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 228.9 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 79.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 258.9 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 64.7 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 79.3 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 258.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 194.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 228.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 129.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 320.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 228.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 129.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 237.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 91.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 194.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 320.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 137.3 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 323.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 194.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 258.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 323.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 158.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 183.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 194.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 237.9 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 228.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 228.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 194.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 258.9 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 317.1 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 194.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 194.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 323.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 274.7 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 79.3 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 258.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 228.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 45.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 228.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrInRh2 (mp-977543) | 0.0025 | 0.000 | 3 |
MnGa2Co (mp-623453) | 0.0025 | 0.118 | 3 |
MnGaRu2 (mp-865140) | 0.0028 | 0.065 | 3 |
VGaRu2 (mp-865586) | 0.0028 | 0.000 | 3 |
TiGeRu2 (mp-865640) | 0.0032 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0054 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0054 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0054 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0054 | 0.211 | 4 |
VGaFeCo (mp-1066581) | 0.0054 | 0.029 | 4 |
GaFe3 (mp-672661) | 0.0047 | 0.038 | 2 |
Rb3Tc (mp-974820) | 0.0047 | 1.260 | 2 |
NaEr3 (mp-976405) | 0.0045 | 0.318 | 2 |
PmAg3 (mp-862878) | 0.0042 | 0.000 | 2 |
EuTe (mp-991027) | 0.0048 | 0.246 | 2 |
Cu (mp-998890) | 0.0054 | 0.037 | 1 |
Kr (mp-974400) | 0.0054 | 0.002 | 1 |
H2 (mp-632250) | 0.0054 | 0.000 | 1 |
Ge (mp-998883) | 0.0054 | 0.340 | 1 |
U (mp-108) | 0.0054 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Re_pv Ag |
Final Energy/Atom-7.4587 eV |
Corrected Energy-29.8350 eV
Uncorrected energy = -29.8350 eV
Corrected energy = -29.8350 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)