Final Magnetic Moment4.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.687 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.860 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg7P6(HO6)4 + MgP2(H4O5)2 + Mg2P2O7 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 203.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 308.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 124.4 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 195.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 142.4 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 81.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 51.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 313.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 243.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 164.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 205.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 224.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 122.3 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 243.1 |
GaN (mp-804) | <1 1 0> | <1 -1 1> | 145.6 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 331.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 154.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 82.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 308.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 290.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 165.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 203.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 224.3 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 195.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 122.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 41.1 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 243.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 165.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 205.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 123.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 -1> | 337.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 205.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 316.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 122.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 201.2 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 243.1 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 163.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 205.7 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 274.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 142.4 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 205.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 163.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 313.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 -1> | 274.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 124.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 143.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 142.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 205.7 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 156.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 142.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NbPCl10 (mp-27787) | 0.5140 | 0.000 | 3 |
Tl2SeO4 (mp-675953) | 0.5112 | 0.011 | 3 |
UPCl10 (mp-540927) | 0.5100 | 0.000 | 3 |
Ni(NF7)2 (mp-558988) | 0.5006 | 0.000 | 3 |
Re2(PCl8)3 (mp-29593) | 0.4832 | 0.000 | 3 |
SiH8(NF3)2 (mp-759722) | 0.4412 | 0.000 | 4 |
TiH8(NF3)2 (mp-696590) | 0.4652 | 0.017 | 4 |
SbPOF8 (mp-560310) | 0.5628 | 0.000 | 4 |
AsSOF9 (mp-556515) | 0.5635 | 0.044 | 4 |
MgPHO9 (mp-720260) | 0.0726 | 0.862 | 4 |
PCl5 (mp-23228) | 0.5773 | 0.000 | 2 |
PCl5 (mp-569410) | 0.5968 | 0.006 | 2 |
InPH5NO5 (mp-764968) | 0.5859 | 0.000 | 5 |
Fe3H10S2NO14 (mp-40778) | 0.6061 | 0.037 | 5 |
NaGaH8(NF3)2 (mp-865095) | 0.6265 | 0.008 | 5 |
InP2H4NO8 (mp-698151) | 0.5828 | 0.237 | 5 |
RbInPHO5 (mp-733729) | 0.5904 | 0.000 | 5 |
AsC4S2Cl2O2F13 (mp-560424) | 0.6111 | 0.226 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv P H O |
Final Energy/Atom-5.1426 eV |
Corrected Energy-63.0249 eV
-63.0249 eV = -61.7110 eV (uncorrected energy) - 1.3138 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)