Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.238 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.575 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/mnm [136] |
Hall-P 4n 2n |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 169.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 275.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 283.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 157.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 169.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 157.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 56.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 69.7 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 278.8 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 172.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 284.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 325.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 196.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 325.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 244.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 275.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.4 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 56.6 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 69.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 339.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 314.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 162.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 196.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 157.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.7 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 226.4 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 169.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 157.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 278.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 196.8 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 196.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 226.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 196.8 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 169.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 122.0 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 283.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 196.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 278.8 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 278.8 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 196.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 196.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.5 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 226.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 278.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 69.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 203.3 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 115.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
189 | 63 | 71 | 0 | 0 | 0 |
63 | 189 | 71 | 0 | 0 | 0 |
71 | 71 | 142 | 0 | 0 | 0 |
0 | 0 | 0 | 78 | 0 | 0 |
0 | 0 | 0 | 0 | 78 | 0 |
0 | 0 | 0 | 0 | 0 | 79 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.7 | -1.2 | -2.8 | 0 | 0 | 0 |
-1.2 | 6.7 | -2.8 | 0 | 0 | 0 |
-2.8 | -2.8 | 9.8 | 0 | 0 | 0 |
0 | 0 | 0 | 12.7 | 0 | 0 |
0 | 0 | 0 | 0 | 12.7 | 0 |
0 | 0 | 0 | 0 | 0 | 12.7 |
Shear Modulus GV68 GPa |
Bulk Modulus KV103 GPa |
Shear Modulus GR64 GPa |
Bulk Modulus KR102 GPa |
Shear Modulus GVRH66 GPa |
Bulk Modulus KVRH102 GPa |
Elastic Anisotropy0.34 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2SnSb4 (mp-675535) | 0.7337 | 0.230 | 3 |
BaLaCl5 (mp-772035) | 0.7349 | 0.062 | 3 |
La2InNi2 (mp-1079757) | 0.7238 | 0.013 | 3 |
Ga3Ru (mp-672204) | 0.1311 | 0.000 | 2 |
Ga3Co (mp-20559) | 0.1559 | 0.000 | 2 |
In3Ir (mp-630976) | 0.1495 | 0.002 | 2 |
In3Ru (mp-607450) | 0.0858 | 0.000 | 2 |
Ga3Os (mp-570844) | 0.1483 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d Fe_pv |
Final Energy/Atom-4.6268 eV |
Corrected Energy-74.0292 eV
-74.0292 eV = -74.0292 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)