Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.449 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZrNi + ZrNi3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 254.1 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 141.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 161.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 229.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 141.8 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 141.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 141.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 254.1 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 0> | 254.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 227.5 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 84.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 254.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 141.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 169.4 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 1> | 141.8 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 0> | 254.1 |
SiC (mp-8062) | <1 1 0> | <1 0 1> | 161.4 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 84.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 169.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 84.7 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 84.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 141.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 254.1 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 84.7 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 254.1 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 84.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 161.4 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 113.8 |
Ga2O3 (mp-886) | <1 0 1> | <1 1 0> | 142.4 |
WS2 (mp-224) | <1 0 0> | <1 1 1> | 182.3 |
NaCl (mp-22862) | <1 0 0> | <1 0 1> | 161.4 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 169.4 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 169.4 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 227.5 |
GaTe (mp-542812) | <1 0 -1> | <0 0 1> | 227.5 |
Ge (mp-32) | <1 0 0> | <0 1 0> | 169.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Ni_pv |
Final Energy/Atom-7.3683 eV |
Corrected Energy-250.5210 eV
-250.5210 eV = -250.5210 eV (uncorrected energy)
|