Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.319 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 0 0> | <0 1 0> | 338.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 211.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 338.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 253.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 186.1 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 211.5 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 190.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 126.9 |
Al (mp-134) | <1 0 0> | <0 1 0> | 338.4 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.5 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 186.1 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 211.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 126.9 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 126.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 338.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 338.4 |
C (mp-66) | <1 1 0> | <0 1 0> | 211.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 338.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 126.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 338.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 296.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 253.8 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 169.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 296.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 253.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 253.8 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 253.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 141.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 120.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 169.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 211.5 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 296.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 296.1 |
C (mp-66) | <1 0 0> | <0 1 0> | 126.9 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 296.1 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 296.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 148.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 148.1 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 211.5 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 211.5 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 211.5 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 253.8 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 211.5 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 253.8 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 148.1 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 211.5 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 186.1 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 338.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 240.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
167 | 49 | 51 | -0 | 0 | 0 |
49 | 172 | 54 | -0 | 0 | 0 |
51 | 54 | 140 | -0 | 0 | 0 |
-0 | -0 | -0 | 42 | 0 | 0 |
0 | 0 | 0 | 0 | 40 | 0 |
0 | 0 | 0 | 0 | 0 | 51 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7 | -1.3 | -2 | 0 | 0 | 0 |
-1.3 | 6.9 | -2.2 | 0 | 0 | 0 |
-2 | -2.2 | 8.7 | 0 | 0 | 0 |
0 | 0 | 0 | 23.8 | 0 | 0 |
0 | 0 | 0 | 0 | 25.1 | 0 |
0 | 0 | 0 | 0 | 0 | 19.6 |
Shear Modulus GV48 GPa |
Bulk Modulus KV87 GPa |
Shear Modulus GR47 GPa |
Bulk Modulus KR87 GPa |
Shear Modulus GVRH48 GPa |
Bulk Modulus KVRH87 GPa |
Elastic Anisotropy0.12 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2GaSn2 (mp-640159) | 0.4600 | 0.000 | 3 |
U3Ga5 (mp-669688) | 0.7326 | 0.219 | 2 |
Mg3Si2 (mp-1075771) | 0.7087 | 0.239 | 2 |
H3W (mp-1078686) | 0.7457 | 0.149 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Sn_d |
Final Energy/Atom-5.8719 eV |
Corrected Energy-117.4382 eV
-117.4382 eV = -117.4382 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)