Final Magnetic Moment5.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.195 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.206 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42m [121] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 170.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 170.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 120.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 286.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 300.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 148.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 297.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 148.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 286.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 148.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 286.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 222.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 170.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 95.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 255.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 297.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 180.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 297.0 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 170.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 255.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 170.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 180.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 297.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 148.5 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 0> | 255.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 255.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 286.7 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 240.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 297.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 180.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 222.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 180.5 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 255.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 300.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 286.7 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 286.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 222.8 |
C (mp-66) | <1 1 0> | <1 0 0> | 180.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 300.8 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 300.8 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 74.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 300.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 300.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 74.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 148.5 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 286.7 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 300.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 95.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.36929 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.47541 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.47541 |
Piezoelectric Modulus ‖eij‖max0.47541 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
15.47 | 0.00 | 0.00 |
0.00 | 14.14 | 0.00 |
0.00 | 0.00 | 14.14 |
Dielectric Tensor εij (total) |
||
---|---|---|
43.47 | 0.00 | 0.00 |
0.00 | 35.21 | 0.00 |
0.00 | 0.00 | 35.21 |
Polycrystalline dielectric constant
εpoly∞
14.58
|
Polycrystalline dielectric constant
εpoly
37.96
|
Refractive Index n3.82 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl3In2Se5 (mp-686102) | 0.2667 | 0.001 | 3 |
Tl3In7Se10 (mp-675519) | 0.2765 | 0.034 | 3 |
TlGaTe2 (mp-3785) | 0.2570 | 0.000 | 3 |
NaAlTe2 (mp-10163) | 0.2701 | 0.000 | 3 |
NaGaTe2 (mp-10164) | 0.2774 | 0.006 | 3 |
MnTl2SnTe4 (mp-569859) | 0.2302 | 0.000 | 4 |
Tl2CdSnTe4 (mp-570076) | 0.2033 | 0.009 | 4 |
K2CdSnSe4 (mp-1079645) | 0.2762 | 0.000 | 4 |
Rb2SnHgTe4 (mp-1080691) | 0.2110 | 0.000 | 4 |
Tl2SnHgTe4 (mp-570051) | 0.2183 | 0.012 | 4 |
TlSe (mp-1836) | 0.3702 | 0.000 | 2 |
TlS (mp-322) | 0.4351 | 0.052 | 2 |
InTe (mp-20320) | 0.3300 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Tl_d Ge_d Te |
Final Energy/Atom-4.0793 eV |
Corrected Energy-34.3228 eV
Uncorrected energy = -32.6348 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -34.3228 eV
|