Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.263 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.549 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 144.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 144.4 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 144.4 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 144.4 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 144.4 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 144.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 144.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BePO4 (mp-760410) | 0.2847 | 0.063 | 3 |
AlPO4 (mp-707977) | 0.3749 | 0.010 | 3 |
AlPO4 (mp-541338) | 0.3687 | 0.012 | 3 |
AlPO4 (mp-555941) | 0.3870 | 0.011 | 3 |
AlPO4 (mp-559145) | 0.3815 | 0.013 | 3 |
Cs2MgSi5O12 (mp-1019610) | 0.7417 | 0.000 | 4 |
SiO2 (mp-600003) | 0.1419 | 0.009 | 2 |
BeF2 (mp-559400) | 0.1177 | 0.002 | 2 |
SiO2 (mp-555556) | 0.1387 | 0.009 | 2 |
CeSe2 (mp-1080363) | 0.1390 | 0.524 | 2 |
CeSe2 (mp-1080863) | 0.1305 | 0.522 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9009 eV |
Corrected Energy-602.5736 eV
-602.5736 eV = -568.8636 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)