Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.265 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.664 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3m [229] |
Hall-I 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-7848) | 0.3470 | 0.000 | 3 |
BePO4 (mp-760410) | 0.1899 | 0.063 | 3 |
AlPO4 (mp-541338) | 0.3454 | 0.012 | 3 |
AlPO4 (mp-555941) | 0.3228 | 0.011 | 3 |
AlPO4 (mp-559145) | 0.3312 | 0.013 | 3 |
Cs2MgSi5O12 (mp-1019610) | 0.7370 | 0.000 | 4 |
SiO2 (mp-639511) | 0.0851 | 0.012 | 2 |
SiO2 (mp-639724) | 0.1051 | 0.011 | 2 |
SiO2 (mp-600098) | 0.1046 | 0.012 | 2 |
SiO2 (mp-17909) | 0.1037 | 0.012 | 2 |
SiO2 (mp-600016) | 0.0970 | 0.011 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9035 eV |
Corrected Energy-602.7636 eV
-602.7636 eV = -569.0537 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|