Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.016 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 280.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 280.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 246.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 215.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 281.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 317.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 277.0 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 277.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 87.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 176.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 174.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 123.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 246.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 140.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 215.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 246.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 348.3 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 277.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 307.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 277.0 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 233.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 130.6 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 130.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 281.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 277.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 348.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 246.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 317.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 246.6 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 336.0 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 168.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 176.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 348.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 277.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 215.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 187.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 317.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 277.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 281.8 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 261.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 277.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 140.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 176.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 130.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 123.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 35.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 246.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 317.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 174.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
2 | 3 | 4 | 0 | 0 | 0 |
3 | 2 | 4 | 0 | 0 | 0 |
4 | 4 | 3 | 0 | 0 | 0 |
0 | 0 | 0 | 1 | 0 | 0 |
0 | 0 | 0 | 0 | 1 | 0 |
0 | 0 | 0 | 0 | 0 | 1 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-624.7 | 365.9 | 339.8 | 0 | 0 | 0 |
365.9 | -624.7 | 339.8 | 0 | 0 | 0 |
339.8 | 339.8 | -538.5 | 0 | 0 | 0 |
0 | 0 | 0 | 706.1 | 0 | 0 |
0 | 0 | 0 | 0 | 706.1 | 0 |
0 | 0 | 0 | 0 | 0 | 760.5 |
Shear Modulus GV1 GPa |
Bulk Modulus KV3 GPa |
Shear Modulus GR-3 GPa |
Bulk Modulus KR3 GPa |
Shear Modulus GVRH-1 GPa |
Bulk Modulus KVRH3 GPa |
Elastic Anisotropy-6.00 |
Poisson's Ratio0.72 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaSb2Au (mp-675224) | 0.7004 | 0.286 | 3 |
LiFeAs (mp-1008927) | 0.6278 | 0.296 | 3 |
Al2Os (mp-7188) | 0.3160 | 0.000 | 2 |
EuPb (mp-20394) | 0.1635 | 0.000 | 2 |
HoHg2 (mp-1063224) | 0.2067 | 0.070 | 2 |
LaAs (mp-20494) | 0.0610 | 0.370 | 2 |
CaZn3 (mp-1094784) | 0.1721 | 0.121 | 2 |
Hg (mp-569289) | 0.0348 | 0.008 | 1 |
Pr (mp-568938) | 0.1030 | 0.086 | 1 |
Sc (mp-1056366) | 0.0466 | 0.110 | 1 |
Pr (mp-1056311) | 0.2607 | 0.086 | 1 |
Ca (mp-1078638) | 0.1121 | 0.019 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv |
Final Energy/Atom-0.9643 eV |
Corrected Energy-0.9643 eV
-0.9643 eV = -0.9643 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)