Final Magnetic Moment31.932 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.311 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.351 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn + MnAu2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 205.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 292.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 123.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 136.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 205.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 214.8 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 227.1 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 227.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 253.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 156.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 97.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 287.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 156.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 164.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 156.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 227.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 328.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 246.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 287.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 175.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 227.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 156.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 156.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 287.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 253.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 58.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 253.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 164.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 195.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 156.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 246.1 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 232.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 328.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 287.1 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 272.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 156.2 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 290.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 292.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 195.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 174.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 123.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 156.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 318.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 232.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMgSnPd (mp-7555) | 0.3867 | 0.000 | 4 |
LiMgSbPt (mp-571584) | 0.3867 | 0.080 | 4 |
TiFeCoSi (mp-998971) | 0.3867 | 0.027 | 4 |
TiFeCoAs (mp-998974) | 0.3867 | 0.134 | 4 |
LiMgSbPd (mp-10179) | 0.3867 | 0.066 | 4 |
BiF3 (mp-557466) | 0.2581 | 0.270 | 2 |
LiMg2 (mp-865939) | 0.2673 | 0.000 | 2 |
YbGa (mp-396) | 0.2932 | 0.000 | 2 |
LuPb2 (mp-11493) | 0.2677 | 0.017 | 2 |
TiMo3 (mp-1017983) | 0.2296 | 0.000 | 2 |
Li8Al3Si5 (mp-30134) | 0.2684 | 0.200 | 3 |
ThInAg2 (mp-862932) | 0.2909 | 0.000 | 3 |
NaY2In (mp-635327) | 0.3095 | 0.508 | 3 |
NaLi5N2 (mp-29929) | 0.2263 | 0.245 | 3 |
GdCdPd2 (mp-866034) | 0.3087 | 0.000 | 3 |
Sc (mp-10641) | 0.2958 | 0.104 | 1 |
Hg (mp-1017981) | 0.3185 | 0.002 | 1 |
Li (mp-567337) | 0.3866 | 0.003 | 1 |
Sb (mp-7761) | 0.3184 | 0.237 | 1 |
Ca (mp-21) | 0.3593 | 0.014 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points38 |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Au |
Final Energy/Atom-7.3774 eV |
Corrected Energy-88.5292 eV
-88.5292 eV = -88.5292 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)