Final Magnetic Moment0.123 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.137 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 279.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 279.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 279.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 93.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 279.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 93.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 186.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 279.1 |
Au (mp-81) | <1 1 1> | <0 0 1> | 93.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 279.1 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 279.1 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 279.1 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 279.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 279.1 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 279.1 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 279.1 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 279.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 279.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 279.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 93.0 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 279.1 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 93.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 279.1 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 279.1 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 93.0 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 279.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm4Si3Pd4 (mp-680578) | 0.7125 | 0.024 | 3 |
Ca2InPt2 (mp-21885) | 0.6868 | 0.000 | 3 |
Ca2InPd2 (mp-20792) | 0.6919 | 0.000 | 3 |
Eu2InPt2 (mp-1095035) | 0.6891 | 0.000 | 3 |
Mg3Ga7Co2 (mp-571626) | 0.7148 | 0.000 | 3 |
K2Au3 (mp-8700) | 0.6827 | 0.000 | 2 |
Rb8Tl11 (mp-542781) | 0.1741 | 0.000 | 2 |
K8Tl11 (mp-569570) | 0.3202 | 0.000 | 2 |
K8In11 (mp-582929) | 0.1102 | 0.000 | 2 |
MgSi2 (mp-1073455) | 0.7191 | 0.199 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv In_d |
Final Energy/Atom-2.1429 eV |
Corrected Energy-81.4300 eV
-81.4300 eV = -81.4300 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)