Final Magnetic Moment1.697 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.677 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd5Si4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 169.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 236.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 242.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 248.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 118.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 124.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 310.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 186.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 169.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 248.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 124.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 136.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 62.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 136.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 133.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 236.3 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 242.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 136.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 310.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 186.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 242.1 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 236.3 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 236.3 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 242.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 310.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 236.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 310.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 248.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 136.0 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 62.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 186.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 169.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 1> | 180.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 62.0 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 169.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 124.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 124.0 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 242.1 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 310.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 62.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 62.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 310.0 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 310.0 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 136.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 124.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 310.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 1> | 133.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 62.0 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 133.4 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 124.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(YbGe)4 (mp-646071) | 0.6936 | 0.032 | 3 |
Pr2Sc3Si4 (mp-568831) | 0.5807 | 0.000 | 3 |
Sc2Re3Si4 (mp-16794) | 0.6999 | 0.000 | 3 |
U2Ti3Si4 (mp-22814) | 0.6718 | 0.021 | 3 |
Ce2Sc3Si4 (mp-505512) | 0.5807 | 0.000 | 3 |
Dy5Si4 (mp-542828) | 0.2537 | 0.018 | 2 |
Ho5Si4 (mp-542829) | 0.2932 | 0.021 | 2 |
Sm5Si4 (mp-567800) | 0.0912 | 0.006 | 2 |
Er5Si4 (mp-568446) | 0.2810 | 0.023 | 2 |
Pr5Si4 (mp-542465) | 0.3653 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Si |
Final Energy/Atom-5.7360 eV |
Corrected Energy-206.4969 eV
-206.4969 eV = -206.4969 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)