material

Fe13Co3

ID:

mp-641526

DOI:

10.17188/1280035


Tags: Iron cobalt (13/3)

Material Details

Final Magnetic Moment
36.743 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.032 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.004 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.04 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Fe3Co + Fe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <1 0 0> 0.000 32.6
Al (mp-134) <1 1 0> <1 1 0> 0.000 46.2
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.000 261.1
MgO (mp-1265) <1 0 0> <1 0 0> 0.000 163.2
BN (mp-984) <0 0 1> <1 1 1> 0.001 169.6
TiO2 (mp-390) <0 0 1> <1 0 0> 0.001 130.6
Cu (mp-30) <1 0 0> <1 0 0> 0.002 65.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.005 163.2
AlN (mp-661) <1 0 1> <1 0 0> 0.011 195.8
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.014 32.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.015 46.2
Ni (mp-23) <1 1 0> <1 1 0> 0.024 138.5
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.026 226.1
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.035 323.1
NaCl (mp-22862) <1 0 0> <1 0 0> 0.041 32.6
NaCl (mp-22862) <1 1 0> <1 1 0> 0.044 46.2
NaCl (mp-22862) <1 1 1> <1 1 1> 0.046 56.5
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.053 293.7
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.053 184.6
C (mp-48) <1 0 1> <1 0 0> 0.061 261.1
TePb (mp-19717) <1 1 0> <1 1 0> 0.068 184.6
TePb (mp-19717) <1 1 1> <1 1 1> 0.070 226.1
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.070 226.1
SiC (mp-7631) <0 0 1> <1 1 1> 0.075 226.1
CdTe (mp-406) <1 1 0> <1 1 0> 0.076 184.6
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.077 323.1
CdTe (mp-406) <1 1 1> <1 1 1> 0.077 226.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.079 32.6
AlN (mp-661) <1 0 0> <1 1 1> 0.081 282.7
SiC (mp-11714) <0 0 1> <1 1 1> 0.084 226.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.084 46.2
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.085 56.5
CdS (mp-672) <1 1 1> <1 0 0> 0.094 261.1
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.095 261.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.097 184.6
InSb (mp-20012) <1 1 1> <1 1 1> 0.099 226.1
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.103 46.2
Al (mp-134) <1 1 1> <1 0 0> 0.109 228.5
C (mp-48) <0 0 1> <1 1 0> 0.115 184.6
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.116 46.2
AlN (mp-661) <0 0 1> <1 1 1> 0.119 226.1
LiF (mp-1138) <1 1 1> <1 0 0> 0.122 228.5
WS2 (mp-224) <0 0 1> <1 1 1> 0.122 169.6
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.123 169.6
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.127 46.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.127 32.6
GaAs (mp-2534) <1 1 0> <1 1 0> 0.135 46.2
GaAs (mp-2534) <1 1 1> <1 1 1> 0.137 56.5
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.138 359.0
ZnO (mp-2133) <1 0 1> <1 1 1> 0.139 339.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
269 140 140 0 0 0
140 271 144 0 0 0
140 144 271 0 0 0
0 0 0 114 0 0
0 0 0 0 117 0
0 0 0 0 0 117
Compliance Tensor Sij (10-12Pa-1)
5.7 -1.9 -1.9 0 0 0
-1.9 5.8 -2.1 0 0 0
-1.9 -2.1 5.8 0 0 0
0 0 0 8.8 0 0
0 0 0 0 8.5 0
0 0 0 0 0 8.5
Shear Modulus GV
96 GPa
Bulk Modulus KV
184 GPa
Shear Modulus GR
88 GPa
Bulk Modulus KR
184 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
184 GPa
Elastic Anisotropy
0.43
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ta2ReRu (mp-977357) 0.0083 0.000 3
LaRe2Ag (mp-631674) 0.0102 0.831 3
EuInAu2 (mp-866021) 0.0092 0.015 3
Li2EuSn (mp-867474) 0.0101 0.000 3
LaInHg2 (mp-867979) 0.0103 0.000 3
VFeCoGe (mp-1063914) 0.0135 0.000 4
TiFeCoSi (mp-998971) 0.0135 0.029 4
MnFeCoGe (mp-1018024) 0.0135 0.007 4
VFeCoAs (mp-1066006) 0.0135 0.221 4
VGaFeCo (mp-1066581) 0.0135 0.029 4
GaFe3 (mp-672661) 0.0129 0.036 2
Rb3Tc (mp-974820) 0.0129 1.248 2
Fe11Co5 (mp-601848) 0.0100 0.000 2
PmAg3 (mp-862878) 0.0118 0.000 2
EuTe (mp-991027) 0.0125 0.246 2
Cu (mp-998890) 0.0135 0.037 1
Kr (mp-974400) 0.0135 0.002 1
H2 (mp-632250) 0.0135 2.271 1
Ge (mp-998883) 0.0135 0.339 1
U (mp-108) 0.0135 0.269 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Fe_pv Co
Final Energy/Atom
-8.2469 eV
Corrected Energy
-131.9500 eV
Uncorrected energy = -131.9500 eV Corrected energy = -131.9500 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 155844
Submitted by
User remarks:
  • Iron cobalt (13/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)