Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.813 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToXeF6 |
Band Gap2.583 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 0> | <0 0 1> | 112.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 223.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 223.9 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 157.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 112.0 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 223.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 223.9 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 157.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 112.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 157.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 112.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 193.1 |
CaCO3 (mp-3953) | <1 1 0> | <0 1 0> | 157.3 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 1> | 193.1 |
SiC (mp-8062) | <1 0 0> | <0 1 1> | 193.1 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 157.3 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 112.0 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 112.0 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 223.9 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 112.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 112.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KU2F9 (mp-669376) | 0.7071 | 0.068 | 3 |
Rb3Nb2S11 (mp-541745) | 0.7236 | 0.000 | 3 |
Rb3Ta2S11 (mp-541975) | 0.7218 | 0.000 | 3 |
BaZrF6 (mp-556738) | 0.5574 | 0.003 | 3 |
K3Nb2Se11 (mp-28428) | 0.7087 | 0.000 | 3 |
Rb2BaNb2Se11 (mp-571293) | 0.6519 | 0.000 | 4 |
Ba2YSn2F11 (mvc-9413) | 0.6620 | 0.078 | 4 |
Ba2YW2F11 (mvc-9958) | 0.7397 | 0.259 | 4 |
VF5 (mp-765975) | 0.7127 | 0.082 | 2 |
UO3 (mp-21858) | 0.6504 | 0.083 | 2 |
VF5 (mp-765782) | 0.6688 | 0.084 | 2 |
XeF6 (mp-560366) | 0.4014 | 0.000 | 2 |
UF5 (mp-1760) | 0.7093 | 0.045 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Xe F |
Final Energy/Atom-2.0358 eV |
Corrected Energy-228.0146 eV
-228.0146 eV = -228.0146 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)