Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.771 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2(PbS2)3 + Bi2S3 |
Band Gap1.133 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 295.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 245.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 242.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 147.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 242.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 295.0 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 312.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 344.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 49.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 242.8 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 312.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 242.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 303.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 121.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 49.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 344.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 303.5 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 1 0> | 121.4 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 0 1> | 245.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 242.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 295.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 49.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 234.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 60.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 196.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 303.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 312.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 49.2 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 182.1 |
TeO2 (mp-2125) | <1 1 0> | <0 1 1> | 312.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 303.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 245.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 245.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 147.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 234.3 |
BN (mp-984) | <0 0 1> | <1 1 1> | 191.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 242.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 60.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 344.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 196.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 49.2 |
Al (mp-134) | <1 1 0> | <0 1 1> | 234.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 312.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 295.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 312.4 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 182.1 |
SiC (mp-7631) | <1 0 1> | <1 1 1> | 191.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 242.8 |
PbS (mp-21276) | <1 1 1> | <0 1 1> | 312.4 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 242.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(CoO2)2 (mvc-12655) | 0.4639 | 0.237 | 3 |
Li2FeF4 (mp-777665) | 0.5714 | 0.074 | 3 |
Mg(WO2)2 (mvc-5982) | 0.5652 | 0.423 | 3 |
Ce2SnSe4 (mp-1006368) | 0.2525 | 0.078 | 3 |
Ca2SnS4 (mp-866539) | 0.5587 | 0.314 | 3 |
FeSb6(Pb2S7)2 (mp-22369) | 0.7063 | 0.041 | 4 |
Li7V(O2F)2 (mp-765831) | 0.6688 | 0.094 | 4 |
MnSb6(Pb2S7)2 (mp-683891) | 0.6365 | 0.008 | 4 |
KCu(BiS2)2 (mp-558063) | 0.5997 | 0.000 | 4 |
AgBi2S3Cl (mp-558368) | 0.7107 | 0.008 | 4 |
Ti3N4 (mp-1080192) | 0.6557 | 0.101 | 2 |
Ca3N2 (mp-568172) | 0.6359 | 0.048 | 2 |
Sc2O3 (mp-558748) | 0.6179 | 0.074 | 2 |
Ti2O3 (mp-776456) | 0.6248 | 0.070 | 2 |
Zr3N4 (mp-277) | 0.6458 | 0.000 | 2 |
Li10Fe3Co2Ni3O16 (mp-779868) | 0.7151 | 0.100 | 5 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.7478 | 0.107 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi Pb_d S |
Final Energy/Atom-4.3973 eV |
Corrected Energy-133.7386 eV
-133.7386 eV = -123.1233 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)