Final Magnetic Moment0.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.611 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 223.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 223.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 250.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 267.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 133.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 223.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 178.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 312.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 223.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 189.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 133.9 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 166.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 178.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 44.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 223.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 312.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 133.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 267.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 223.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 178.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 250.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 312.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 223.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 166.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 223.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 133.9 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 312.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 1 0> | 250.2 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 223.2 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 223.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 312.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 178.5 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 283.8 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 267.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 312.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 223.2 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 178.5 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 178.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 44.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 312.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 250.2 |
Au (mp-81) | <1 0 0> | <0 0 1> | 312.5 |
Au (mp-81) | <1 1 0> | <0 1 0> | 250.2 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 312.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 312.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 312.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 189.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 178.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 178.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 44.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y6Te2Pd (mp-642293) | 0.2315 | 0.000 | 3 |
Y6AgTe2 (mp-642238) | 0.2681 | 0.000 | 3 |
Y6Te2Rh (mp-21621) | 0.3138 | 0.000 | 3 |
Sc6AgTe2 (mp-30203) | 0.3642 | 0.012 | 3 |
Lu6AgTe2 (mp-569414) | 0.2625 | 0.000 | 3 |
Ti2Se (mp-680576) | 0.4276 | 0.005 | 2 |
Ta2P (mp-22477) | 0.3899 | 0.000 | 2 |
Ta2As (mp-672222) | 0.4179 | 0.015 | 2 |
Dy2Te (mp-505682) | 0.4111 | 0.000 | 2 |
Zr2Se (mp-22642) | 0.3912 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Cu_pv Te |
Final Energy/Atom-4.7792 eV |
Corrected Energy-175.4254 eV
Uncorrected energy = -172.0494 eV
Composition-based energy adjustment (-0.422 eV/atom x 8.0 atoms) = -3.3760 eV
Corrected energy = -175.4254 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)