Final Magnetic Moment0.435 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.105 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.139 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O3 + DyVO4 + Dy2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 177.3 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 177.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 204.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 144.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 102.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 144.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 102.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 144.7 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 102.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 144.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 177.3 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 177.3 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 144.7 |
Ge (mp-32) | <1 1 1> | <1 1 1> | 177.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y2Fe2O7 (mvc-3489) | 0.0629 | 0.000 | 3 |
Gd2V2O7 (mp-773164) | 0.0805 | 0.159 | 3 |
Sc2Ge2O7 (mp-757450) | 0.0636 | 0.015 | 3 |
Lu2Mn2O7 (mp-19153) | 0.0712 | 0.000 | 3 |
Er2Mn2O7 (mp-19256) | 0.0054 | 0.000 | 3 |
Mn2Hg2SF6 (mp-600275) | 0.2473 | 0.465 | 4 |
Zn2Hg2OF6 (mp-17972) | 0.2392 | 0.000 | 4 |
Mn2Hg2SF6 (mp-556900) | 0.2316 | 0.465 | 4 |
Ni2Hg2OF6 (mp-540834) | 0.3188 | 0.000 | 4 |
Ca2Ta2O6F (mp-14560) | 0.1346 | 0.076 | 4 |
GdTi2CdO6F (mp-695048) | 0.3284 | 0.142 | 5 |
YbTi2CdO6F (mp-677010) | 0.2567 | 0.121 | 5 |
NdTi2CdO6F (mp-677732) | 0.3037 | 0.159 | 5 |
Ca2Nd2Nb3FeO14 (mvc-16570) | 0.3758 | 0.111 | 5 |
EuTi2CdO6F (mp-684730) | 0.2636 | 0.099 | 5 |
NaYbTiNbO6F (mp-684861) | 0.5196 | 0.065 | 6 |
NaPrTiNbO6F (mp-42897) | 0.5698 | 0.035 | 6 |
NaEuTiNbO6F (mp-43048) | 0.4755 | 0.021 | 6 |
NaCeTiNbO6F (mp-43055) | 0.5461 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.5692 | 0.038 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Dy_3 V_pv O |
Final Energy/Atom-7.9895 eV |
Corrected Energy-192.1880 eV
Uncorrected energy = -175.7700 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -192.1880 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)