Final Magnetic Moment0.503 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.123 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiSeO3 |
Band Gap2.917 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 156.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 173.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 173.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 156.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 173.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 148.5 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 173.7 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 156.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 -1> | 173.7 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 156.5 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 -1> | 173.7 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 148.5 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 156.5 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 156.5 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 156.5 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 148.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn6O5F7 (mp-764108) | 0.5339 | 0.060 | 3 |
Mn3Se3O10 (mp-505203) | 0.5235 | 0.000 | 3 |
Fe2Se2O7 (mp-561440) | 0.5165 | 0.505 | 3 |
Zn(MoO2)4 (mvc-154) | 0.4945 | 0.136 | 3 |
Fe4As5O13 (mp-505012) | 0.5047 | 0.000 | 3 |
Ta2MnZnO8 (mvc-13175) | 0.5615 | 0.078 | 4 |
Ta4Mn2Zn3O16 (mvc-12018) | 0.5648 | 0.047 | 4 |
MnNb2ZnO8 (mvc-15048) | 0.5554 | 0.082 | 4 |
Li2Mn3(SeO3)4 (mp-773608) | 0.4494 | 0.000 | 4 |
LiFe(SeO3)2 (mp-566507) | 0.4809 | 0.000 | 4 |
SnO2 (mvc-5316) | 0.6222 | 0.223 | 2 |
V7O13 (mp-715598) | 0.7224 | 0.020 | 2 |
Li2VH2OF5 (mp-861531) | 0.6477 | 0.068 | 5 |
Li2VH2OF5 (mp-770536) | 0.6716 | 0.062 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv Se O |
Final Energy/Atom-5.0927 eV |
Corrected Energy-475.7521 eV
-475.7521 eV = -407.4181 eV (uncorrected energy) - 34.6240 eV (MP Advanced Correction) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)