Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.404 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsP(HO2)2 + CsPO3 |
Band Gap5.585 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 294.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 186.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 294.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 93.0 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 93.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 294.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 93.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 278.9 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 186.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 294.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 93.0 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 140.2 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 128.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 128.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 220.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 93.0 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 186.0 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 278.9 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 118.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 93.0 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 220.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 186.0 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 278.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 220.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 278.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 220.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 220.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 93.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 294.2 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 257.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 210.0 |
BN (mp-984) | <1 1 1> | <0 1 1> | 237.1 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 128.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 294.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 220.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 278.9 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 186.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 140.2 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 294.2 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 278.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 294.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 294.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 220.6 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 93.0 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 186.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 220.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 93.0 |
NdGaO3 (mp-3196) | <1 1 0> | <0 1 0> | 186.0 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 278.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 294.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HClO4 (mp-706301) | 0.6778 | 0.019 | 3 |
PSN9 (mp-1020739) | 0.6911 | 0.281 | 3 |
RbH3(SO4)2 (mp-733612) | 0.4418 | 0.000 | 4 |
RbP(HO2)2 (mp-722348) | 0.4893 | 0.074 | 4 |
CsHSeO4 (mp-24141) | 0.3348 | 0.000 | 4 |
HS2IO8 (mp-765597) | 0.5395 | 0.000 | 4 |
HSeNO4 (mp-696797) | 0.5219 | 1.026 | 4 |
Ti2O7 (mp-656850) | 0.7423 | 0.501 | 2 |
KPHO3F (mp-758619) | 0.5897 | 0.000 | 5 |
RbPHO3F (mp-774810) | 0.3989 | 0.000 | 5 |
Rb2PH3SeO8 (mp-686677) | 0.4797 | 0.005 | 5 |
CsPH3O3F (mp-574928) | 0.5080 | 0.009 | 5 |
Rb2PH3SeO8 (mp-753854) | 0.5176 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv P H O |
Final Energy/Atom-6.1595 eV |
Corrected Energy-169.9795 eV
-169.9795 eV = -160.1475 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)