Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.274 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.130 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK4H6C2O9 + H2O + C |
Band Gap5.179 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 300.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 280.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 300.3 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 285.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 176.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 88.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 271.9 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 285.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 280.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 286.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 155.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 168.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 181.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 242.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 271.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 144.6 |
GaN (mp-804) | <1 0 0> | <1 -1 -1> | 217.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 176.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 198.5 |
GaN (mp-804) | <1 1 1> | <1 -1 0> | 267.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 244.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 271.9 |
KCl (mp-23193) | <1 0 0> | <1 -1 1> | 204.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 -1> | 217.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 180.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 271.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 181.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 310.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 285.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 242.6 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 211.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 168.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 181.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 240.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 180.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 116.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 176.5 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 267.3 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 163.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 198.5 |
CdS (mp-672) | <1 1 1> | <0 1 -1> | 204.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 168.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 168.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 116.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 285.7 |
Te2W (mp-22693) | <1 0 0> | <1 -1 0> | 200.4 |
Te2W (mp-22693) | <1 0 1> | <1 -1 0> | 200.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 264.7 |
YVO4 (mp-19133) | <0 0 1> | <1 -1 1> | 204.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 194.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H2C3O4 (mp-559232) | 0.6027 | 0.261 | 3 |
H4C5O2 (mp-995218) | 0.6075 | 0.235 | 3 |
HCO (mp-995234) | 0.5601 | 0.265 | 3 |
Be(N3O7)2 (mp-30141) | 0.5818 | 0.055 | 3 |
C4O5F6 (mp-556192) | 0.6072 | 0.131 | 3 |
H8C3(NO)4 (mp-708965) | 0.6078 | 0.570 | 4 |
H9C5NO5 (mp-558863) | 0.5647 | 0.268 | 4 |
K2SN2O5 (mp-560434) | 0.5088 | 0.229 | 4 |
AlC3(NCl2)3 (mp-607454) | 0.5993 | 0.000 | 4 |
K2SN2O5 (mp-1019784) | 0.5584 | 0.230 | 4 |
ZnH8C4(NO3)2 (mp-655017) | 0.6100 | 0.584 | 5 |
GdH7C2SO8 (mp-559733) | 0.6323 | 0.030 | 5 |
C2SClO4F3 (mp-555625) | 0.6125 | 0.209 | 5 |
KH3C2S2O (mp-555919) | 0.3995 | 0.183 | 5 |
ZnH8C4(NO3)2 (mp-601243) | 0.6084 | 0.584 | 5 |
B2H10C2NClO3 (mp-554977) | 0.6160 | 0.158 | 6 |
NaH18C9I(NO)3 (mp-720100) | 0.6726 | 0.612 | 6 |
PH8C2SNO2 (mp-561476) | 0.6873 | 0.119 | 6 |
B2H10C2NClO3 (mp-554598) | 0.5430 | 0.158 | 6 |
H6C3SN3O2F3 (mp-555728) | 0.6065 | 0.366 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv H C O |
Final Energy/Atom-5.9429 eV |
Corrected Energy-111.0934 eV
Uncorrected energy = -106.9714 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -111.0934 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)