material

Ba4Y(CuO3)3

ID:

mp-643409

DOI:

10.17188/1280309


Tags: Barium yttrium copper oxide (1/.25/.75/2.25)

Material Details

Final Magnetic Moment
0.680 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.390 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiF (mp-1138) <1 1 1> <1 1 1> 0.000 115.5
LiF (mp-1138) <1 1 0> <1 1 0> 0.000 94.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.000 66.7
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.001 115.5
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.001 94.3
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.001 66.7
C (mp-66) <1 0 0> <1 0 0> 0.007 333.3
MgO (mp-1265) <1 1 0> <1 1 0> 0.007 282.8
Ge (mp-32) <1 1 0> <1 1 0> 0.008 94.3
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.008 115.5
Ge (mp-32) <1 0 0> <1 0 0> 0.009 66.7
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.009 115.5
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.018 282.8
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.020 333.3
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.036 282.8
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.037 333.3
Si (mp-149) <1 0 0> <1 0 0> 0.056 266.7
InSb (mp-20012) <1 1 0> <1 1 0> 0.060 188.6
CdTe (mp-406) <1 1 0> <1 1 0> 0.076 188.6
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.089 133.3
Ni (mp-23) <1 1 0> <1 1 0> 0.140 188.6
Mg (mp-153) <1 0 0> <1 1 0> 0.150 282.8
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.154 333.3
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.193 266.7
KCl (mp-23193) <1 0 0> <1 0 0> 0.214 333.3
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.248 188.6
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.260 94.3
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.262 266.7
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.263 200.0
Al (mp-134) <1 1 1> <1 1 1> 0.265 115.5
Al (mp-134) <1 1 0> <1 1 0> 0.270 94.3
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.280 266.7
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.284 188.6
Al (mp-134) <1 0 0> <1 0 0> 0.285 66.7
Ga2O3 (mp-886) <0 1 0> <1 1 0> 0.287 282.8
Mg (mp-153) <1 1 1> <1 0 0> 0.288 266.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.296 333.3
SiC (mp-8062) <1 0 0> <1 0 0> 0.300 333.3
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.327 133.3
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.330 133.3
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.332 94.3
GaP (mp-2490) <1 0 0> <1 0 0> 0.344 266.7
BN (mp-984) <1 0 1> <1 0 0> 0.350 266.7
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.357 133.3
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.374 333.3
CdS (mp-672) <1 1 1> <1 0 0> 0.378 266.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.388 94.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.410 66.7
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.415 94.3
ZnO (mp-2133) <0 0 1> <1 0 0> 0.418 333.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
195 58 58 0 0 0
58 195 58 0 0 0
58 58 195 0 0 0
0 0 0 42 0 0
0 0 0 0 42 0
0 0 0 0 0 42
Compliance Tensor Sij (10-12Pa-1)
5.9 -1.4 -1.4 0 0 0
-1.4 5.9 -1.4 0 0 0
-1.4 -1.4 5.9 0 0 0
0 0 0 23.9 0 0
0 0 0 0 23.9 0
0 0 0 0 0 23.9
Shear Modulus GV
52 GPa
Bulk Modulus KV
104 GPa
Shear Modulus GR
50 GPa
Bulk Modulus KR
104 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
104 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba4Yb(CuO3)3 (mp-653337) 0.0776 0.000 4
Ba4Ce(CuO3)3 (mp-1096779) 0.0562 0.018 4
Ba4Cu3PbO9 (mp-1023127) 0.0356 0.037 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Y_sv Cu_pv O
Final Energy/Atom
-6.1931 eV
Corrected Energy
-223.2072 eV
-223.2072 eV = -210.5660 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 65549
Submitted by
User remarks:
  • Barium yttrium copper oxide (1/.25/.75/2.25)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)