@article{Besserguenev1997, author = "Besserguenev, A.V. and Fogg, A.M. and Francis, R.J. and Price, S.J. and O'Hare, D. and Isupov, V.P. and Tolochko, B.P.", title = "Synthesis and structure of the gibbsite intercalation compounds (Li Al2 (O H)6) X (X = Cl, Br, N O3) and (Li Al2 (O H)6) Cl (H2 O) using synchrotron X-ray and neutron powder diffraction", journal = "Chemistry of Materials", year = "1997", volume = "9", pages = "241-247", ASTM_id = "CMATEX" }