Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.659 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 270.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 225.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 135.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 288.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 80.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 45.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 119.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 268.2 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 126.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 169.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 84.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 236.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 101.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 90.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 128.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 160.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 80.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 135.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 288.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 67.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 169.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 208.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 238.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 270.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 208.1 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 180.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 270.6 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 101.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 240.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 240.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 268.2 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 268.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 149.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 96.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 238.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 327.8 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 238.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 80.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 16.0 |
Al (mp-134) | <1 1 0> | <1 0 1> | 67.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 144.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 208.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 203.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.1 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 135.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeSiHRu (mp-604496) | 0.2940 | 0.003 | 4 |
CePRuO (mp-21372) | 0.3939 | 0.000 | 4 |
CeNiAsO (mp-1079455) | 0.3555 | 0.529 | 4 |
CeAsRuO (mp-1080105) | 0.3693 | 0.000 | 4 |
CaNiGeH (mp-1095188) | 0.3153 | 0.030 | 4 |
InBi (mp-23313) | 0.7036 | 0.000 | 2 |
NaSr7Cu8(SF)8 (mp-603276) | 0.7055 | 0.007 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Co Ge_d H |
Final Energy/Atom-5.8832 eV |
Corrected Energy-47.4235 eV
Uncorrected energy = -47.0655 eV
Composition-based energy adjustment (-0.179 eV/atom x 2.0 atoms) = -0.3580 eV
Corrected energy = -47.4235 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)