Final Magnetic Moment1.986 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.708 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.481 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImmm [71] |
Hall-I 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 155.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 155.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 109.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 310.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 155.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 258.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 155.2 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 109.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 242.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 206.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 310.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 258.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 206.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 109.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 218.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 258.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 258.6 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 258.6 |
Al (mp-134) | <1 0 0> | <0 1 1> | 242.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 206.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 310.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 258.6 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 206.9 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 206.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 186.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 218.8 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 103.4 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 109.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 51.7 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 186.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 155.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 109.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 109.4 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 51.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 310.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 310.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 51.7 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 155.2 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 109.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 51.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 258.6 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 258.6 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 155.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 109.4 |
Ga2O3 (mp-886) | <1 1 1> | <0 0 1> | 258.6 |
Au (mp-81) | <1 1 0> | <0 1 0> | 218.8 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 109.4 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 242.0 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 310.3 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 109.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.00000 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.67 | 0.00 | 0.00 |
0.00 | 2.44 | 0.00 |
0.00 | 0.00 | 2.51 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.51 | 0.00 | 0.00 |
0.00 | 5.30 | 0.00 |
0.00 | 0.00 | 7.39 |
Polycrystalline dielectric constant
εpoly∞
2.54
|
Polycrystalline dielectric constant
εpoly
6.40
|
Refractive Index n1.59 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaMg(CO2)2 (mp-1080511) | 0.7467 | 0.506 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Cs_sv V_pv H Cl O |
Final Energy/Atom-4.4580 eV |
Corrected Energy-102.5251 eV
Uncorrected energy = -98.0771 eV
Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV
Composition-based energy adjustment (-1.700 eV/atom x 1.0 atoms) = -1.7000 eV
Corrected energy = -102.5251 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)