Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.065 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.401 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density18.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToUIr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 302.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 -1> | 302.8 |
AlN (mp-661) | <0 0 1> | <1 -1 0> | 269.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.5 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 269.8 |
AlN (mp-661) | <1 1 1> | <1 -1 1> | 285.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 262.6 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 204.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 272.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 247.1 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 152.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 278.0 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 143.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 242.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 262.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 247.1 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 232.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 242.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 287.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 278.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 260.5 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 285.2 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 260.5 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 228.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 262.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 262.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 -1 -1> | 189.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 151.1 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 232.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 232.7 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 269.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 262.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 232.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 216.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 216.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 216.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 216.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 185.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 339.7 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 121.1 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 173.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 237.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 226.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 237.7 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 315.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 154.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 332.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 142.6 |
BN (mp-984) | <1 1 1> | <1 1 0> | 302.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 154.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2Fe3Si4 (mp-29111) | 0.5921 | 0.010 | 3 |
Nb4Cr2Si5 (mp-3276) | 0.6283 | 0.034 | 3 |
Pr2CdCu2 (mp-861595) | 0.6938 | 0.000 | 3 |
CsMg6V (mp-1098079) | 0.6876 | 0.614 | 3 |
Mg3Ga7Co2 (mp-571626) | 0.6820 | 0.000 | 3 |
MgSi (mp-1073852) | 0.6212 | 0.186 | 2 |
U3Ga5 (mp-669688) | 0.6012 | 0.219 | 2 |
Re2Si (mp-669547) | 0.6256 | 0.311 | 2 |
Mg4Si3 (mp-1074279) | 0.6209 | 0.177 | 2 |
Mg3Si2 (mp-1075771) | 0.5828 | 0.239 | 2 |
Bi (mp-1078637) | 0.7021 | 0.097 | 1 |
Si (mp-1079649) | 0.6029 | 0.426 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Ir |
Final Energy/Atom-10.1301 eV |
Corrected Energy-162.0815 eV
-162.0815 eV = -162.0815 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)