material

FeBiO3

ID:

mp-645159

DOI:

10.17188/1280505


Tags: Bismuth ferrate - orthorhombic Bismuth ferrate(III) - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.767 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Bi2O3 + Fe2O3
Band Gap
1.569 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 162895 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaN (mp-804) <1 1 1> <0 1 1> 0.007 214.4
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.008 303.6
Mg (mp-153) <1 1 0> <0 1 0> 0.011 86.8
Mg (mp-153) <0 0 1> <0 0 1> 0.015 157.4
WS2 (mp-224) <1 1 1> <0 0 1> 0.027 157.4
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.028 31.5
SrTiO3 (mp-4651) <1 1 0> <1 1 0> 0.029 62.7
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.041 31.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.044 94.4
ZnO (mp-2133) <1 1 0> <1 0 0> 0.050 90.4
BaF2 (mp-1029) <1 0 0> <1 1 0> 0.052 313.3
WS2 (mp-224) <1 1 0> <0 0 1> 0.052 157.4
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.061 55.1
CdWO4 (mp-19387) <1 0 0> <0 1 0> 0.064 216.9
KCl (mp-23193) <1 1 0> <0 1 0> 0.064 173.5
CdS (mp-672) <0 0 1> <0 1 0> 0.067 303.6
ZrO2 (mp-2858) <0 0 1> <1 1 0> 0.070 250.7
DyScO3 (mp-31120) <1 1 0> <1 1 0> 0.074 62.7
LiF (mp-1138) <1 1 0> <0 0 1> 0.075 94.4
PbSe (mp-2201) <1 0 0> <1 1 0> 0.077 313.3
DyScO3 (mp-31120) <0 1 1> <0 1 1> 0.077 53.6
WS2 (mp-224) <1 0 1> <1 0 1> 0.079 275.5
DyScO3 (mp-31120) <1 1 1> <1 1 1> 0.079 70.1
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.090 280.5
Ge (mp-32) <1 1 0> <0 0 1> 0.093 94.4
C (mp-48) <1 0 0> <1 0 0> 0.095 135.7
TiO2 (mp-390) <1 0 0> <1 0 1> 0.099 110.2
TbScO3 (mp-31119) <0 1 1> <0 1 1> 0.099 53.6
CsI (mp-614603) <1 1 0> <0 1 0> 0.102 86.8
CaF2 (mp-2741) <1 1 0> <0 1 0> 0.104 43.4
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.106 43.4
LiGaO2 (mp-5854) <1 0 0> <0 1 1> 0.108 107.2
YAlO3 (mp-3792) <0 1 0> <0 1 0> 0.110 347.0
GaSb (mp-1156) <1 0 0> <1 1 0> 0.116 313.3
C (mp-66) <1 0 0> <1 0 0> 0.119 316.6
BN (mp-984) <0 0 1> <0 0 1> 0.129 188.8
Mg (mp-153) <1 1 1> <0 1 1> 0.134 214.4
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.135 43.4
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.136 283.2
GaAs (mp-2534) <1 1 0> <0 0 1> 0.139 94.4
AlN (mp-661) <1 0 1> <1 0 0> 0.140 90.4
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.141 55.1
TbScO3 (mp-31119) <1 1 1> <1 1 1> 0.141 70.1
SrTiO3 (mp-4651) <1 0 1> <0 1 1> 0.149 53.6
CsI (mp-614603) <1 0 0> <1 1 0> 0.151 62.7
GaP (mp-2490) <1 1 0> <0 1 0> 0.151 43.4
TbScO3 (mp-31119) <1 1 0> <1 1 0> 0.152 62.7
CdSe (mp-2691) <1 0 0> <1 1 0> 0.153 313.3
GaN (mp-804) <1 1 0> <0 1 0> 0.155 86.8
TiO2 (mp-390) <0 0 1> <1 0 1> 0.157 220.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
242 121 119 0 0 0
121 243 119 0 0 0
119 119 255 0 0 0
0 0 0 78 0 0
0 0 0 0 60 0
0 0 0 0 0 90
Compliance Tensor Sij (10-12Pa-1)
6.1 -2.1 -1.9 0 0 0
-2.1 6.1 -1.8 0 0 0
-1.9 -1.8 5.7 0 0 0
0 0 0 12.9 0 0
0 0 0 0 16.6 0
0 0 0 0 0 11.1
Shear Modulus GV
71 GPa
Bulk Modulus KV
162 GPa
Shear Modulus GR
69 GPa
Bulk Modulus KR
162 GPa
Shear Modulus GVRH
70 GPa
Bulk Modulus KVRH
162 GPa
Elastic Anisotropy
0.12
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CrBiO3 (mp-774313) 0.1359 0.011 3
CaHfO3 (mp-754853) 0.1408 0.000 3
CrBiO3 (mp-566058) 0.0982 0.011 3
CaRuO3 (mp-20947) 0.1411 0.000 3
NaMgF3 (mp-2955) 0.1557 0.000 3
Ca2CrIrO6 (mvc-5785) 0.1463 0.000 4
Ca2FeIrO6 (mvc-5784) 0.1626 0.000 4
Ca2SnIrO6 (mvc-5666) 0.1565 0.067 4
Ca4Zr3TaO12 (mp-756837) 0.1458 0.033 4
Ca2FeSbO6 (mp-24970) 0.1570 0.000 4
Pb3O4 (mp-636813) 0.7095 0.038 2
U2S3 (mp-672690) 0.7255 0.173 2
Al2O3 (mp-642363) 0.7441 0.280 2
Mn5O8 (mp-18922) 0.7399 0.009 2
Mn5O8 (mp-715008) 0.7470 0.009 2
CaLaMgTaO6 (mp-684801) 0.2279 0.000 5
LiLaNdSbO6 (mp-776091) 0.2526 0.006 5
CaLaCrMoO6 (mvc-9974) 0.2353 0.014 5
CaLaCrWO6 (mvc-9998) 0.2428 0.056 5
CaLaMnRuO6 (mp-690556) 0.2558 0.135 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Polycrystalline bismuth ferrite (BiFeO3 or BFO) thin films were prepared by chemical solution deposition to explore the impact of processing conditions including annealing temperature, percent excess [...]
The target composition of 0.71BiFeO30.29BaTiO3+xwt% MnO2 (abbreviated as BFBT-Mnx%, x=0.1, 0.3, 0.6, 0.9, 1.2%) was produced by ball milling precursors of high purity (>99%) oxide or carbonate [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition FeBiO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv Bi O
Final Energy/Atom
-6.2402 eV
Corrected Energy
-144.1633 eV
-144.1633 eV = -124.8038 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 168321
  • 162895
Submitted by
User remarks:
  • Bismuth ferrate - orthorhombic

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)