Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.321 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbBiO4 + Bi2O3 |
Band Gap1.341 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnc2 [30] |
HallP 2 2bc |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 154.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 154.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 154.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 340.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 126.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 154.7 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 126.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 247.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 122.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 278.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 244.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 174.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 216.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 309.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 216.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 61.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 216.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 154.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 92.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 278.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 309.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 340.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 154.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 154.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 154.7 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 278.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 216.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 309.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 123.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 247.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 185.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 92.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 30.9 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 154.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 309.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 216.5 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 244.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 278.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 278.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 309.3 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 126.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 278.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 61.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 216.5 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 216.5 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 122.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 30.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 154.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCr2O6 (mvc-13364) | 0.7419 | 0.358 | 3 |
Ti3(BiO3)4 (mp-723064) | 0.6150 | 0.001 | 3 |
Ti3(BiO3)4 (mp-23427) | 0.7086 | 0.006 | 3 |
Ti3(BiO3)4 (mp-558277) | 0.6261 | 0.007 | 3 |
La2Nb2N2O5 (mp-775929) | 0.7406 | 0.055 | 4 |
SrNb2Bi2O9 (mp-23614) | 0.6789 | 0.000 | 4 |
Na2Te4MoO12 (mp-559249) | 0.7037 | 0.000 | 4 |
Na2Te4WO12 (mp-562125) | 0.7372 | 0.000 | 4 |
Ag2Mo3SeO12 (mp-566624) | 0.7455 | 0.009 | 4 |
UO3 (mp-616580) | 0.7046 | 0.134 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Bi O |
Final Energy/Atom-7.2525 eV |
Corrected Energy-354.2259 eV
Uncorrected energy = -333.6159 eV
Composition-based energy adjustment (-0.687 eV/atom x 30.0 atoms) = -20.6100 eV
Corrected energy = -354.2259 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)