Final Magnetic Moment0.080 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.253 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIn3Co + TmIn3 + Co |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 126.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 119.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 315.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 273.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 279.6 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 239.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 298.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 273.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 168.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 179.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 189.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 105.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 105.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 231.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 357.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 279.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 357.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 42.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 210.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 237.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 168.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 179.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 84.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 179.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 336.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 357.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 294.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 84.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 237.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 158.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 294.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 237.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 336.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 237.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 105.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 42.1 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 223.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 294.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 84.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 63.1 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 237.2 |
GaSe (mp-1943) | <1 1 1> | <1 1 0> | 237.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 189.4 |
BN (mp-984) | <1 1 0> | <1 0 1> | 298.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 315.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 336.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 273.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 378.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 119.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er2Ga8Co (mp-985468) | 0.1711 | 0.004 | 3 |
U2Ga8Ru (mp-21493) | 0.1369 | 0.020 | 3 |
Ho2Ga8Co (mp-4513) | 0.1759 | 0.003 | 3 |
Nd2In8Co (mp-1095457) | 0.1678 | 0.009 | 3 |
Ho2In8Co (mp-1095593) | 0.1046 | 0.011 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 In_d Co |
Final Energy/Atom-3.7141 eV |
Corrected Energy-40.8553 eV
Uncorrected energy = -40.8553 eV
Corrected energy = -40.8553 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)