Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.599 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.818 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 138.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 194.6 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 204.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 324.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 230.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 323.2 |
GaAs (mp-2534) | <1 0 0> | <1 -1 1> | 269.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 329.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 277.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 273.7 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 207.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 138.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 264.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 230.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 323.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 323.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 273.7 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 0> | 318.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 194.6 |
KCl (mp-23193) | <1 0 0> | <1 -1 -1> | 282.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 -1> | 272.3 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 273.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 323.2 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 1> | 269.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 329.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 209.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 324.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 138.5 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 209.7 |
LiF (mp-1138) | <1 0 0> | <1 -1 1> | 269.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 324.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 323.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 230.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 209.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 324.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 259.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 230.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 324.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 329.6 |
Ag (mp-124) | <1 0 0> | <1 -1 0> | 238.6 |
Ag (mp-124) | <1 1 0> | <1 -1 0> | 318.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 230.8 |
BN (mp-984) | <0 0 1> | <0 1 1> | 273.7 |
BN (mp-984) | <1 0 0> | <1 1 1> | 254.6 |
BN (mp-984) | <1 0 1> | <1 -1 -1> | 282.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 138.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 -1 0> | 238.6 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 323.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuSeO4 (mp-554109) | 0.5556 | 0.003 | 3 |
Fe4As2O11 (mp-31803) | 0.4613 | 0.136 | 3 |
Ni4P4O15 (mp-585202) | 0.5308 | 0.059 | 3 |
V4As2O13 (mp-32447) | 0.5525 | 0.000 | 3 |
Ni4P4O15 (mp-705427) | 0.5249 | 0.059 | 3 |
Li2Mn2(PO4)3 (mp-762616) | 0.4910 | 0.018 | 4 |
Li2Cr2P2O9 (mp-761438) | 0.4425 | 0.211 | 4 |
MgV6(FeO6)4 (mvc-14468) | 0.4941 | 0.235 | 4 |
Li2V(PO4)2 (mp-540312) | 0.4617 | 0.056 | 4 |
LiNi2(PO4)3 (mp-697786) | 0.4930 | 0.278 | 4 |
FeO2 (mvc-11999) | 0.6306 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.5878 | 0.351 | 2 |
VO2 (mp-777469) | 0.6354 | 0.038 | 2 |
VO2 (mvc-6918) | 0.5769 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6140 | 0.387 | 2 |
ZnCoNiP2O9 (mvc-8275) | 0.5380 | 0.237 | 5 |
Li2MnV(PO4)3 (mp-771376) | 0.5027 | 0.030 | 5 |
Li2MnV(PO4)3 (mp-770134) | 0.4521 | 0.028 | 5 |
LiCrPO4F (mp-770575) | 0.4935 | 0.069 | 5 |
K2LiTi2(AsO5)2 (mp-772826) | 0.5358 | 0.107 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6038 | 0.173 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6065 | 0.003 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.6437 | 0.114 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5962 | 0.041 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.4784 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6368 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv Mg_pv V_pv O |
Final Energy/Atom-6.9215 eV |
Corrected Energy-245.4277 eV
Uncorrected energy = -221.4877 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-1.700 eV/atom x 6.0 atoms) = -10.2000 eV
Corrected energy = -245.4277 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)