material

Eu2O3

ID:

mp-647924

DOI:

10.17188/1280786


Tags: Europium oxide Europium(III) oxide Europium oxide (2/3)

Material Details

Final Magnetic Moment
3.923 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-3.139 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.040 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.56 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Eu2O3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 8056 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 200.3
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 294.0
AlN (mp-661) <0 0 1> <1 0 -1> 170.5
AlN (mp-661) <1 0 0> <1 0 0> 326.7
AlN (mp-661) <1 0 1> <1 1 1> 143.5
AlN (mp-661) <1 1 0> <1 0 -1> 340.9
CeO2 (mp-20194) <1 0 0> <1 0 0> 294.0
CeO2 (mp-20194) <1 1 0> <1 0 -1> 170.5
GaAs (mp-2534) <1 0 0> <0 0 1> 263.4
BaF2 (mp-1029) <1 0 0> <1 0 0> 163.3
BaF2 (mp-1029) <1 1 0> <1 0 0> 228.7
BaF2 (mp-1029) <1 1 1> <1 0 -1> 284.1
GaN (mp-804) <0 0 1> <1 0 0> 326.7
GaN (mp-804) <1 0 0> <0 0 1> 316.1
GaN (mp-804) <1 0 1> <1 0 0> 228.7
GaN (mp-804) <1 1 0> <1 0 0> 294.0
SiO2 (mp-6930) <0 0 1> <1 0 0> 228.7
SiO2 (mp-6930) <1 0 0> <1 0 0> 294.0
SiO2 (mp-6930) <1 1 0> <1 0 0> 98.0
SiO2 (mp-6930) <1 1 1> <1 0 0> 261.3
KCl (mp-23193) <1 0 0> <1 0 0> 163.3
KCl (mp-23193) <1 1 0> <1 0 0> 228.7
KCl (mp-23193) <1 1 1> <1 0 -1> 284.1
DyScO3 (mp-31120) <0 1 0> <1 0 -1> 170.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 228.7
DyScO3 (mp-31120) <1 1 0> <0 0 1> 263.4
InAs (mp-20305) <1 0 0> <1 0 0> 228.7
InAs (mp-20305) <1 1 0> <1 0 0> 163.3
ZnSe (mp-1190) <1 0 0> <0 0 1> 263.4
KTaO3 (mp-3614) <1 0 0> <0 0 1> 210.7
KTaO3 (mp-3614) <1 1 0> <1 0 0> 261.3
CdS (mp-672) <0 0 1> <0 0 1> 105.4
CdS (mp-672) <1 0 0> <1 0 0> 196.0
CdS (mp-672) <1 1 0> <1 0 -1> 340.9
CdS (mp-672) <1 1 1> <1 0 0> 261.3
LiF (mp-1138) <1 0 0> <0 0 1> 263.4
LiF (mp-1138) <1 1 0> <1 0 0> 261.3
Te2W (mp-22693) <0 0 1> <1 0 0> 294.0
Te2W (mp-22693) <1 1 0> <1 0 -1> 113.6
Te2W (mp-22693) <1 1 1> <1 0 0> 228.7
YVO4 (mp-19133) <0 0 1> <1 0 0> 261.3
YVO4 (mp-19133) <1 0 0> <1 0 -1> 227.3
YVO4 (mp-19133) <1 0 1> <0 0 1> 210.7
TePb (mp-19717) <1 0 0> <0 0 1> 210.7
Te2Mo (mp-602) <0 0 1> <1 0 1> 66.8
Te2Mo (mp-602) <1 0 0> <1 0 -1> 56.8
Te2Mo (mp-602) <1 0 1> <1 0 0> 228.7
Te2Mo (mp-602) <1 1 0> <1 0 -1> 284.1
Ag (mp-124) <1 0 0> <1 0 0> 359.3
Ag (mp-124) <1 1 0> <1 0 -1> 227.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
144 90 62 0 11 0
90 183 67 0 6 0
62 67 199 0 4 0
0 0 0 27 0 -1
11 6 4 0 45 0
0 0 0 -1 0 61
Compliance Tensor Sij (10-12Pa-1)
10.7 -4.5 -1.8 0 -1.9 0
-4.5 8.2 -1.3 0 0.1 0
-1.8 -1.3 6 0 0.1 0
0 0 0 37.6 0 0.9
-1.9 0.1 0.1 0 22.7 0
0 0 0 0.9 0 16.5
Shear Modulus GV
47 GPa
Bulk Modulus KV
107 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
104 GPa
Shear Modulus GVRH
44 GPa
Bulk Modulus KVRH
106 GPa
Elastic Anisotropy
0.66
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zr2N2O (mp-775863) 0.4061 0.071 3
Zr2N2O (mp-755368) 0.4028 0.059 3
Hf2N2O (mp-755314) 0.4146 0.073 3
Hf2N2O (mp-760052) 0.3539 0.100 3
Zr2N2O (mp-776273) 0.3497 0.066 3
Li7VO5F (mp-764407) 0.6109 0.067 4
Li7VO5F (mp-764775) 0.5162 0.067 4
Li7Mn(OF)3 (mp-764343) 0.5567 0.085 4
Li7Co(OF)3 (mp-763913) 0.6040 0.101 4
Li8MnO5F (mp-767026) 0.6087 0.027 4
Ho2O3 (mp-558336) 0.2359 0.046 2
Y2O3 (mp-558573) 0.2285 0.048 2
Dy2O3 (mp-555574) 0.2427 0.043 2
Tb2O3 (mp-2457) 0.2273 0.040 2
Er2O3 (mp-2460) 0.2371 0.048 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Novel -SiAlON:Eu2+-based yellow oxynitride phosphors with the formula Sr0.375xEux2+Si12mnAlm+nOnN16n (m=0.75, n=x=0.0040.04) have been prepared by firing the powder mixture of SrSi2, -Si3 [...]
Eu suppressed the grain size from approximately 100 m for pure Eu2O3 to 6 m when the specimens were fired at 1800 C in air for one hour. Three at % substitution of Ta for Eu suppressed the grain si [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Eu2O3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Eu O
Final Energy/Atom
-9.8036 eV
Corrected Energy
-153.3744 eV
-153.3744 eV = -147.0538 eV (uncorrected energy) - 6.3206 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 631461
  • 631453
  • 659184
  • 8056
Submitted by
User remarks:
  • Europium(III) oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)