Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.139 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.211 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + SiCl4 + SiO2 + C + Os |
Band Gap2.559 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 1> | 299.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 263.7 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 213.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 197.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 329.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 329.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 293.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 293.3 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 299.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 329.6 |
BN (mp-984) | <0 0 1> | <1 1 1> | 212.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 197.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 275.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 329.6 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 275.1 |
SiC (mp-7631) | <1 0 0> | <1 1 -1> | 141.6 |
C (mp-66) | <1 1 0> | <1 0 1> | 199.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 329.6 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 263.7 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 263.7 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 197.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 197.8 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 293.3 |
C (mp-48) | <1 1 0> | <0 1 0> | 275.1 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 213.0 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 263.7 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 329.6 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 -1> | 114.6 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 1> | 199.3 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 1> | 299.0 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 293.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 329.6 |
Au (mp-81) | <1 1 1> | <1 0 1> | 299.0 |
C (mp-48) | <1 0 0> | <1 1 1> | 212.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 263.7 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 263.7 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 263.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 329.6 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 329.6 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 195.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 299.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 -1 1> | 159.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 197.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 1> | 222.5 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 197.8 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 195.6 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 275.1 |
ZnO (mp-2133) | <0 0 1> | <1 0 1> | 299.0 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 263.7 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 329.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Os(CO)4 (mp-679947) | 0.7291 | 0.226 | 3 |
Os(CO)4 (mp-640748) | 0.6873 | 0.214 | 3 |
Ru(CO)4 (mp-652407) | 0.6748 | 0.221 | 3 |
Ru4C14O13 (mp-653243) | 0.7391 | 0.250 | 3 |
Os6C19O20 (mp-648157) | 0.6820 | 0.225 | 3 |
Os3C12(IO6)2 (mp-621944) | 0.5961 | 0.170 | 4 |
Fe4Pb(CO)16 (mp-652092) | 0.6507 | 0.707 | 4 |
Ru3C10(NO6)2 (mp-680280) | 0.6387 | 0.286 | 4 |
Fe2Os(CO)12 (mp-683792) | 0.6606 | 0.532 | 4 |
Os2Pt(CO)9 (mp-650695) | 0.6516 | 0.220 | 4 |
P2Os4C15O13F6 (mp-667424) | 0.6631 | 0.304 | 5 |
H2Ru6C18SO20 (mp-720807) | 0.5986 | 0.183 | 5 |
HOs6C18S2O19 (mp-707923) | 0.6668 | 0.203 | 5 |
Mn2SnC9ClO9 (mp-699647) | 0.7259 | 0.603 | 5 |
PRu4C15O14F3 (mp-667397) | 0.5621 | 0.268 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Os_pv C Cl O |
Final Energy/Atom-7.2451 eV |
Corrected Energy-262.0077 eV
-262.0077 eV = -253.5802 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)